Torreya
Woods sold under several trade names often come from one genus. These 2 share the genus Torreya, so they are close relatives and frequent substitutes for each other.
0 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| California torreya (nutmeg)Torreya californica | 599 lbf* | 32.3 lb/ft³ |
| Florida torreya (nutmeg)Torreya taxifolia | 645 lbf* | 33.9 lb/ft³ |