genus
Trichospermum
Woods sold under several trade names often come from one genus. These 2 share the genus Trichospermum, so they are close relatives and frequent substitutes for each other.
0 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| MaouliTrichospermum richii | 395 lbf* | 25.1 lb/ft³ |
| Trichospermum ikutaiTrichospermum ikutai | 423 lbf* | 26.0 lb/ft³ |