genus
Trophis
Woods sold under several trade names often come from one genus. These 2 share the genus Trophis, so they are close relatives and frequent substitutes for each other.
1 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| RamónTrophis spp. | 770 lbf | 40.0 lb/ft³ |
| White ramoonTrophis racemosa | 1,658 lbf* | 48.9 lb/ft³ |