genus
Ulmus
Woods sold under several trade names often come from one genus. These 10 share the genus Ulmus, so they are close relatives and frequent substitutes for each other.
3 of 10 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| American elmUlmus americana | 830 lbf | 35.0 lb/ft³ |
| Cedar elmUlmus crassifolia | 1,419 lbf* | 45.5 lb/ft³ |
| Chinese elmUlmus parvifolia | 1,152 lbf* | 41.3 lb/ft³ |
| English elmUlmus procera | 1,152 lbf* | 41.3 lb/ft³ |
| Japanese elmUlmus davidiana | 1,152 lbf* | 41.3 lb/ft³ |
| Rock elmUlmus thomasii | 1,320 lbf | 44.1 lb/ft³ |
| September elmUlmus serotina | 1,152 lbf* | 41.3 lb/ft³ |
| Siberian elmUlmus pumila | 1,152 lbf* | 41.3 lb/ft³ |
| Slippery elmUlmus rubra | 860 lbf | 37.1 lb/ft³ |
| Winged elmUlmus alata | 1,475 lbf* | 46.4 lb/ft³ |