genus
Vatairea
Woods sold under several trade names often come from one genus. These 4 share the genus Vatairea, so they are close relatives and frequent substitutes for each other.
4 of 4 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Angelim-amargosoVatairea sericea | 2,167 lbf | 56.2 lb/ft³ |
| Bitter AngelimVatairea spp. | 1,250 lbf | 46.0 lb/ft³ |
| Faveira-amargosaVatairea paraensis | 2,174 lbf | 62.2 lb/ft³ |
| Faveira-amargosaVatairea guianensis | 1,532 lbf | 51.8 lb/ft³ |