genus
Vernicia
Woods sold under several trade names often come from one genus. These 2 share the genus Vernicia, so they are close relatives and frequent substitutes for each other.
0 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Mu oil treeVernicia montana | 423 lbf* | 26.0 lb/ft³ |
| Tungoil treeVernicia fordii | 479 lbf* | 27.5 lb/ft³ |