genus
Vitex
Woods sold under several trade names often come from one genus. These 9 share the genus Vitex, so they are close relatives and frequent substitutes for each other.
3 of 9 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| BarsVitex cofassus | 1,725 lbf* | 49.9 lb/ft³ |
| Chinese chastetreeVitex negundo | 1,054 lbf* | 39.6 lb/ft³ |
| FiddlewoodVitex spp. | 1,160 lbf | 43.0 lb/ft³ |
| HiguerilloVitex divaricata | 1,309 lbf* | 43.8 lb/ft³ |
| Lilac chastetreeVitex agnus-castus | 1,363 lbf* | 44.7 lb/ft³ |
| MolaveVitex spp. | 1,255 lbf | 50.0 lb/ft³ |
| Simpleleaf chastetreeVitex trifolia | 1,309 lbf* | 43.8 lb/ft³ |
| Smallflower chastetreeVitex parviflora | 2,139 lbf* | 55.1 lb/ft³ |
| VitexVitex doniana | 680 lbf | 29.8 lb/ft³ |