Wood Record

genus

Vochysia

Woods sold under several trade names often come from one genus. These 5 share the genus Vochysia, so they are close relatives and frequent substitutes for each other.

4 of 5 carry a published Janka test.

WoodJankaDensity
QuarubaVochysia guianensis1,427 lbf40.1 lb/ft³
QuarubaVochysia maxima976 lbf36.0 lb/ft³
QuarubaVochysia obidensis1,179 lbf38.0 lb/ft³
QuarubaVochysia ferruginea608 lbf*30.0 lb/ft³
YemeriVochysia spp.605 lbf36.0 lb/ft³