Woods sold under several trade names often come from one genus. These 7 share the genus Zanthoxylum, so they are close relatives and frequent substitutes for each other.
1 of 7 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Common pricklyashZanthoxylum americanum | 1,152 lbf* | 41.3 lb/ft³ |
| Dotted pricklyashZanthoxylum punctatum | 2,963 lbf* | 64.1 lb/ft³ |
| Hercules' clubZanthoxylum clava-herculis | 1,203 lbf* | 42.1 lb/ft³ |
| Maminha-de-porcaZanthoxylum rhoifolium = Zanthoxylum regnelianum | 791 lbf | 37.5 lb/ft³ |
| Prickly yellowZanthoxylum caribaeum | 1,923 lbf* | 52.4 lb/ft³ |
| West Indian satinwoodZanthoxylum flavum | 2,448 lbf* | 58.7 lb/ft³ |
| White pricklyashZanthoxylum martinicense | 832 lbf* | 35.5 lb/ft³ |