Wood Record

Is idígbo wood toxic?

A published occupational source reports one effect for idígbo. That is a record of what has happened to people working the wood. It is not a dose, and it is not a prediction for any one person.

Reported effects

  • skin irritation

How strong is this link?

The botanical name matched the source entry, so this record is about this species.

The source entry is filed under "Idigbo #".

Is it safe for a cutting board?

This site does not certify any wood as food safe. No open source makes that judgement species by species, and inventing one would be the unsourced assertion this site exists to avoid.

What the record supports is narrower: a published occupational source reports an effect for idígbo, so treat it with more care than a wood with no such report. Most reported effects come from breathing the dust while machining, and not from finished contact. A reader who reacts to the dust should not assume the finished surface is a problem, and a reader with a known sensitivity should assume nothing at all.

All wood dust

The IARC classifies wood dust as a Group 1 human carcinogen. That applies to every species, including the ones with no entry on this page. Extract at the tool and wear a mask.

Sources

  • DFG, List of MAK and BAT Values 2025, WoodsCC BY 4.0
  • HSE Woodworking Information Sheet 30 (rev 1), Toxic woods, Table 2OGL v3.0
  • IARC Monographs on the Evaluation of Carcinogenic Risks to Humans, Volume 100C, wood dustclassification cited as a fact; the monograph text is (c) WHO/IARC and is not reproduced

Idígbo properties · Every wood with a reported effect