Is striped maple wood toxic?
A published occupational source reports one effect for striped maple. That is a record of what has happened to people working the wood. It is not a dose, and it is not a prediction for any one person.
Reported effects
- reduced lung function
How strong is this link?
A source entry for the genus matched. The report belongs to the genus, and this species may differ from its relatives.
The source entry is filed under "Maple".
Is it safe for a cutting board?
This site does not certify any wood as food safe. No open source makes that judgement species by species, and inventing one would be the unsourced assertion this site exists to avoid.
What the record supports is narrower: a published occupational source reports an effect for striped maple, so treat it with more care than a wood with no such report. Most reported effects come from breathing the dust while machining, and not from finished contact. A reader who reacts to the dust should not assume the finished surface is a problem, and a reader with a known sensitivity should assume nothing at all.
All wood dust
The IARC classifies wood dust as a Group 1 human carcinogen. That applies to every species, including the ones with no entry on this page. Extract at the tool and wear a mask.
Sources
- HSE Woodworking Information Sheet 30 (rev 1), Toxic woods, Table 2OGL v3.0
- IARC Monographs on the Evaluation of Carcinogenic Risks to Humans, Volume 100C, wood dustclassification cited as a fact; the monograph text is (c) WHO/IARC and is not reproduced
Striped maple properties · Every wood with a reported effect