1,785 species. 571 carry a published Janka test. A species with no test says so.

1,785 matching species · Estimates are marked with an asterisk. Images may show a related species; see credits.

Wood species and selected properties
WoodRegionWood typeJanka hardnessDensity
Martinique sweetleaf

Symplocos martinicensis

Genus image · Cirad · Public domain
Range not recordedhardwood1,152 lbf*41.3 lb/ft³*
Marupá

Simarouba amara

Cirad · Public domain
Tropical Americahardwood452 lbf27.5 lb/ft³
Tropical Americahardwood360 lbf25.0 lb/ft³
Matamatá

Eschweilera coriacea

Cirad · Public domain
Tropical Americahardwood2,467 lbf56.2 lb/ft³
Matamatá

Eschweilera grandiflora = Eschweilera cf fracta

Cirad · Public domain
Tropical Americahardwood1,995 lbf53.1 lb/ft³
Matamatá

Eschweilera pedicellata = Eschweilera longipes

Cirad · Public domain
Tropical Americahardwood2,410 lbf61.2 lb/ft³
Matamatá / sapucaia-amargosa

Lecythis idatimon

Cirad · Public domain
Tropical Americahardwood2,341 lbf60.4 lb/ft³*
Matayba apetala

Matayba apetala

Genus image · Cirad · Public domain
Range not recordedhardwood1,538 lbf*47.3 lb/ft³*
Mate

Ilex paraguariensis

Genus image · Cirad · Public domain
Range not recordedhardwood960 lbf*38.0 lb/ft³*
Mati

Ficus tinctoria

Cirad · Public domain
Range not recordedhardwood791 lbf*34.7 lb/ft³*
Mayten

Maytenus boaria

Genus image · Cirad · Public domain
Range not recordedhardwood1,538 lbf*47.3 lb/ft³*
Mbarika

Isoberlinia schaffleri

Genus image · Cirad · Public domain
Africahardwood1,420 lbf50.0 lb/ft³
Mecrusse

Androstachys johnsonii

Cirad · Public domain
Africahardwood2,540 lbf55.0 lb/ft³
Medang

Litsea spp.

Genus image · Cirad · Public domain
Oceaniahardwood562 lbf31.0 lb/ft³
Melancieira

Alexa grandiflora

Cirad · Public domain
Tropical Americahardwood1,424 lbf46.4 lb/ft³*
Melastoma sanguineum

Melastoma sanguineum

Genus image · Cirad · Public domain
Range not recordedhardwood1,007 lbf*38.8 lb/ft³*
Mengkulang

Heritiera spp.

Genus image · Cirad · Public domain
Asiahardwood1,230 lbf42.0 lb/ft³
Merbau

Intsia spp.

Genus image · Cirad · Public domain
Asiahardwood1,500 lbf50.0 lb/ft³
Merkus Pine

Pinus merkusii

Cirad · Public domain
Asiasoftwood620 lbf43.0 lb/ft³
Merpauh

Swintonia spp.

Genus image · Cirad · Public domain
Asiahardwood1,075 lbf46.0 lb/ft³
Mersawa

Anisoptera spp.

Genus image · Cirad · Public domain
Asiahardwood1,290 lbf40.0 lb/ft³
Range not recordedhardwood1,475 lbf*46.4 lb/ft³*
Mesecheues

Canarium hirsutum

Genus image · Cirad · Public domain
Range not recordedhardwood960 lbf*38.0 lb/ft³*
Mexican blue oak

Quercus oblongifolia

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Range not recordedhardwood1,363 lbf*44.7 lb/ft³*
Mexican cypress

Cupressus lustianica

Africasoftwood460 lbf32.0 lb/ft³
Mexican pinyon pine

Pinus cembroides

Genus image · Cirad · Public domain
Range not recordedsoftwood599 lbf*32.3 lb/ft³*
Mexican plum

Prunus mexicana

Genus image · Cirad · Public domain
Range not recordedhardwood832 lbf*35.5 lb/ft³*
Mexican sycamore

Platanus mexicana

Genus image · Cirad · Public domain
Range not recordedhardwood791 lbf*34.7 lb/ft³*
Mexican white oak

Quercus polymorpha

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Miich era ngebard, guiana chestnut

Pachira aquatica

Cirad · Public domain
Range not recordedhardwood753 lbf*33.9 lb/ft³*
Milktree

Sapium laurocerasus

Range not recordedhardwood509 lbf*28.2 lb/ft³*
Milkwood

Tabernaemontana citrifolia

Genus image · Cirad · Public domain
Range not recordedhardwood832 lbf*35.5 lb/ft³*
Mimosa

Albizia julibrissin

Genus image · Cirad · Public domain
Range not recordedhardwood875 lbf*36.3 lb/ft³*
Miraúba

Mouriri collocarpa

Cirad · Public domain
Tropical Americahardwood4,032 lbf68.0 lb/ft³
Missanda

Erythrophleum ivorense

Cirad · Public domain
Africahardwood2,930 lbf56.0 lb/ft³
Miyabe maple

Acer miyabei

Genus image · Cirad · Public domain
Range not recordedhardwood832 lbf*35.5 lb/ft³*
Africasoftwood645 lbf*34.0 lb/ft³
Moabi

Baillonella toxisperma

Cirad · Public domain
Africahardwood2,210 lbf*55.0 lb/ft³
Mockernut hickory

Carya alba

Genus image · Cirad · Public domain
North Americahardwood1,970 lbf50.3 lb/ft³
Molave

Vitex spp.

Genus image · Cirad · Public domain
Asiahardwood1,255 lbf50.0 lb/ft³
Monjoleiro

Senegalia polyphylla = Acacia polyphylla

Genus image · Cirad · Public domain
Tropical Americahardwood1,093 lbf46.2 lb/ft³
Monkeypod

Pithecellobium dulce

Genus image · Cirad · Public domain
Range not recordedhardwood1,538 lbf*47.3 lb/ft³*
Monkeypuzzle tree

Araucaria araucana

Genus image · Cirad · Public domain
Range not recordedsoftwood766 lbf*38.0 lb/ft³*
Range not recordedsoftwood576 lbf*31.5 lb/ft³*
Mora

Mora spp.

Genus image · Cirad · Public domain
Tropical Americahardwood2,300 lbf62.0 lb/ft³
Morototó

Schefflera morototoni

Cirad · Public domain
Tropical Americahardwood789 lbf30.7 lb/ft³*
Moth pepper

Piper blattarum

Genus image · Cirad · Public domain
Range not recordedhardwood714 lbf*33.1 lb/ft³*
Range not recordedhardwood1,255 lbf*43.0 lb/ft³*
Mountain graygum

Eucalyptus goniocalyx

Genus image · Cirad · Public domain
Range not recordedhardwood2,287 lbf*56.9 lb/ft³*
North Americasoftwood680 lbf31.5 lb/ft³
Mountain immortelle

Erythrina poeppigiana

Genus image · Cirad · Public domain
Range not recordedhardwood321 lbf*22.8 lb/ft³*
Mountain maple

Acer spicatum

Genus image · Cirad · Public domain
Range not recordedhardwood832 lbf*35.5 lb/ft³*
Mountain sandalwood

Santalum paniculatum

Genus image · Cirad · Public domain
Range not recordedhardwood1,852 lbf*51.5 lb/ft³*
Range not recordedhardwood641 lbf*31.5 lb/ft³*
Mountain soursop

Annona montana

Genus image · Cirad · Public domain
Range not recordedhardwood753 lbf*33.9 lb/ft³*
Mtambara

Cephalosphaera usambarensis

Adolf Engler · Public domain
Africahardwood740 lbf37.0 lb/ft³
Mtundu

Brachystegia spiciformis

Genus image · Cirad · Public domain
Africahardwood1,830 lbf51.0 lb/ft³
Mu oil tree

Vernicia montana

Genus image · Cirad · Public domain
Range not recordedhardwood423 lbf*26.0 lb/ft³*
Mucilage manjack

Cordia sulcata

Genus image · Cirad · Public domain
Range not recordedhardwood641 lbf*31.5 lb/ft³*
Mueri

Pygeum africanum

Africahardwood1,860 lbf45.0 lb/ft³
Muhimbi

Cynometra alexandri

Genus image · Cirad · Public domain
Africahardwood2,975 lbf54.0 lb/ft³
Muhuhu

Brachylaena hutchinsii

Cirad · Public domain
Africahardwood2,190 lbf58.0 lb/ft³
Muiracatiara

Astronium ulei

Genus image · Cirad · Public domain
Tropical Americahardwood1,684 lbf55.9 lb/ft³*
Muiracatiara-rajada

Astronium lecointei

Cirad · Public domain
Tropical Americahardwood2,051 lbf61.3 lb/ft³*
Muirapixuna

Chamaecrista scleroxylon = Cassia scleroxylon

Genus image · Cirad · Public domain
Tropical Americahardwood3,435 lbf84.1 lb/ft³*
Muiratinga

Maquira sclerophylla

Cirad · Public domain
Tropical Americahardwood1,389 lbf43.8 lb/ft³*
Muirungi

Casearia battiscombei

Genus image · Cirad · Public domain
Africahardwood720 lbf40.0 lb/ft³
Mukulungu

Autranella congolensis

Cirad · Public domain
Africahardwood2,779 lbf*60.0 lb/ft³
Mulga

Acacia aneura

Genus image · Cirad · Public domain
Range not recordedhardwood3,749 lbf*71.5 lb/ft³*
Mullein nightshade

Solanum donianum

Genus image · Cirad · Public domain
Range not recordedhardwood542 lbf*29.1 lb/ft³*
Muneco

Cordia borinquensis

Genus image · Cirad · Public domain
Range not recordedhardwood1,788 lbf*50.7 lb/ft³*
Muninga

Pterocarpus angolensis

Genus image · Cirad · Public domain
Africahardwood1,480 lbf41.0 lb/ft³
Murraya koenigii

Murraya koenigii

Genus image · Cirad · Public domain
Range not recordedhardwood1,658 lbf*48.9 lb/ft³*
Mururé

Brosimum gaudichaudii

Genus image · Cirad · Public domain
Tropical Americahardwood3,036 lbf56.8 lb/ft³
Mururé

Brosimum acutifolium subsp interjectum

Cirad · Public domain
Tropical Americahardwood1,120 lbf42.1 lb/ft³*
Musine

Croton megalocarpus

Genus image · Cirad · Public domain
Africahardwood1,350 lbf44.0 lb/ft³
Musizi

Maesopsis eminii

Cirad · Public domain
Africahardwood600 lbf30.0 lb/ft³
Muttonwood

Turpinia occidentalis

Cirad · Public domain
Range not recordedhardwood679 lbf*32.3 lb/ft³*
Muwa

Julbernardia globiflora

Genus image · Cirad · Public domain
Africahardwood2,470 lbf60.0 lb/ft³
Myrtle oak

Quercus myrtifolia

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Naio

Myoporum sandwicense

Genus image · Cirad · Public domain
Range not recordedhardwood2,139 lbf*55.1 lb/ft³*
Naked albizia

Albizia carbonaria

Genus image · Cirad · Public domain
Range not recordedhardwood1,007 lbf*38.8 lb/ft³*
Nannyberry

Viburnum lentago

Wikidata via Wikimedia Commons · Public domain
Range not recordedhardwood1,658 lbf*48.9 lb/ft³*
Range not recordedhardwood1,309 lbf*43.8 lb/ft³*
Nargusta

Termi nalia amazonia

Tropical Americahardwood1,855 lbf50.0 lb/ft³
Narra

Pterocarpus indicus

Cirad · Public domain
Asiahardwood1,202 lbf40.0 lb/ft³
Narrow-leafed ash

Fraxinus angustifolia

Genus image · Cirad · Public domain
Range not recordedhardwood1,007 lbf*38.8 lb/ft³*
Range not recordedhardwood423 lbf*26.0 lb/ft³*
Narrowleaf red ironbark

Eucalyptus crebra

Genus image · Cirad · Public domain
Range not recordedhardwood2,692 lbf*61.3 lb/ft³*
Nectandra membranacea

Nectandra membranacea

Genus image · Cirad · Public domain
Range not recordedhardwood875 lbf*36.3 lb/ft³*
Nectandra turbacensis

Nectandra turbacensis

Genus image · Cirad · Public domain
Range not recordedhardwood1,103 lbf*40.5 lb/ft³*
Needlewood

Schlma spp.

Asiahardwood1,245 lbf43.0 lb/ft³
Neem

Azadirachta spp.

Genus image · Ton Rulkens · CC BY-SA
Asiahardwood1,460 lbf40.0 lb/ft³
Neem

Azadirachta indica

J.M.Garg · CC BY 3.0
Range not recordedhardwood1,852 lbf*51.5 lb/ft³*
Negra lora

Matayba domingensis

Genus image · Cirad · Public domain
Range not recordedhardwood2,139 lbf*55.1 lb/ft³*
Nemoca

Ocotea moschata

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Nemoca cimarrona

Ocotea spathulata

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Range not recordedhardwood608 lbf*30.7 lb/ft³*
Netleaf oak

Quercus rugosa

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*