Wood Record

All wood species

1,785 species. 571 carry a published Janka test. A species with no test says so.

1,785 matching species · Estimates are marked with an asterisk. Images may show a related species; see credits.

Wood species and selected properties
WoodRegionWood typeJanka hardnessDensity
Pau marfim

Balfourodendron riedelianum

Cirad · Public domain
Tropical Americahardwood2,367 lbf*57.7 lb/ft³*
Pau-amarelo

Euxylophora paraensis

Tropical Americahardwood2,168 lbf50.6 lb/ft³
Pau-branco

Drypetes variabilis

Cirad · Public domain
Tropical Americahardwood2,518 lbf55.9 lb/ft³*
Pau-de-jangada

Apeiba echinata

Genus image · Cirad · Public domain
Tropical Americahardwood558 lbf26.7 lb/ft³*
Pau-jacaré

Laetia procera

Cirad · Public domain
Tropical Americahardwood2,053 lbf52.4 lb/ft³
Pau-ponga

Tachigali sp.

Genus image · Cirad · Public domain
Tropical Americahardwood1,019 lbf36.2 lb/ft³
Pau-santo

Zollernia paraensis

Tropical Americahardwood3,261 lbf78.7 lb/ft³
Paulownia

Paulownia tomentosa

Genus image · Neitram · CC BY-SA 4.0
Asiahardwood235 lbf*19.7 lb/ft³*
Pawpaw

Asimina triloba

Scott Bauer, USDA · Public domain
Range not recordedhardwood509 lbf*28.2 lb/ft³*
Range not recordedhardwood832 lbf*35.5 lb/ft³*
Peachleaf willow

Salix amygdaloides

Genus image · G-Lignum · CC0
Range not recordedhardwood451 lbf*26.7 lb/ft³*
Pear hawthorn

Crataegus calpodendron

Genus image · Cirad · Public domain
Range not recordedhardwood1,725 lbf*49.9 lb/ft³*
Pecan hickory

Carya illinoinensis

Genus image · Cirad · Public domain
North Americahardwood1,820 lbf46.1 lb/ft³
Peepul tree

Ficus religiosa

Genus image · Cirad · Public domain
Range not recordedhardwood679 lbf*32.3 lb/ft³*
Peltophorum pterocarpum

Peltophorum pterocarpum

Cirad · Public domain
Range not recordedhardwood1,363 lbf*44.7 lb/ft³*
Pengua

Macaranga mappa

Genus image · Cirad · Public domain
Range not recordedhardwood423 lbf*26.0 lb/ft³*
Pepperleaf sweetwood

Licaria triandra

Genus image · Cirad · Public domain
Range not recordedhardwood1,923 lbf*52.4 lb/ft³*
Pequiá

Caryocar villosum

Cirad · Public domain
Tropical Americahardwood1,133 lbf48.7 lb/ft³
Pequiarana

Caryocar glabrum

Cirad · Public domain
Tropical Americahardwood1,642 lbf48.7 lb/ft³
Perepat

Sonneratia spp.

Asiahardwood1,078 lbf*40.1 lb/ft³*
Pericopsis mooniana

Pericopsis mooniana

Genus image · Cirad · Public domain
Range not recordedhardwood2,530 lbf*59.6 lb/ft³*
Peroba

Aspidosperma macrocarpon

Genus image · Cirad · Public domain
Tropical Americahardwood1,852 lbf48.7 lb/ft³
Peroba de campos

Paratecoma peroba

Cirad · Public domain
Tropical Americahardwood1,600 lbf46.0 lb/ft³
Peroba rosa

Aspidosperma spp., peroba group

Genus image · Cirad · Public domain
Tropical Americahardwood1,730 lbf51.5 lb/ft³*
Peronia

Ormosia krugii

Genus image · Cirad · Public domain
Range not recordedhardwood753 lbf*33.9 lb/ft³*
Range not recordedhardwood2,210 lbf*55.9 lb/ft³*
Persian Lilac

Melia azedarach

Cirad · Public domain
Asiahardwood832 lbf*36.0 lb/ft³
Persimmon

Diospyros kaki

Genus image · Cirad · Public domain
Range not recordedhardwood1,725 lbf*49.9 lb/ft³*
Perupok

Lophopetalum spp.

Genus image · Cirad · Public domain
Asiahardwood791 lbf*35.0 lb/ft³
Peruvian almond

Terminalia oblonga

Cirad · Public domain
Range not recordedhardwood1,788 lbf*50.7 lb/ft³*
Range not recordedhardwood1,203 lbf*42.1 lb/ft³*
Range not recordedhardwood2,139 lbf*55.1 lb/ft³*
Range not recordedhardwood1,363 lbf*44.7 lb/ft³*
Pigeonberry

Hirtella triandra

Genus image · Cirad · Public domain
Range not recordedhardwood1,990 lbf*53.3 lb/ft³*
Pignut hickory

Carya glabra

Genus image · Cirad · Public domain
North Americahardwood2,140 lbf52.4 lb/ft³
Pillarwood

Cassipourea malosana

Genus image · Cirad · Public domain
Africahardwood1,450 lbf47.0 lb/ft³
Pilon

Hyeronima spp.

Tropical Americahardwood1,700 lbf50.7 lb/ft³*
Pin cherry

Prunus pensylvanica

Genus image · Cirad · Public domain
Range not recordedhardwood832 lbf*35.5 lb/ft³*
Pin oak

Quercus palustris

Wikimedia Commons · Public domain
North Americahardwood1,510 lbf44.1 lb/ft³
Pinchot juniper

Juniperus pinchotii

Genus image · Cirad · Public domain
Range not recordedsoftwood645 lbf*33.9 lb/ft³*
Pinho-cuiabano

Schizolobium parahyba = Schizolobium amazonicum

Cirad · Public domain
Tropical Americahardwood586 lbf29.3 lb/ft³
Pink flame tree

Brachychiton discolor

SAplants · CC BY-SA 4.0
Range not recordedhardwood216 lbf*19.0 lb/ft³*
Pink ivory

Berchemia zeyheri

Genus image · Cirad · Public domain
Africahardwood2,963 lbf*64.1 lb/ft³*
Pink shower

Cassia grandis

Genus image · Cirad · Public domain
Range not recordedhardwood1,852 lbf*51.5 lb/ft³*
Pink tabebuia

Tabebuia pallida

Cirad · Public domain
Range not recordedhardwood1,054 lbf*39.6 lb/ft³*
Pink trumpet-tree

Tabebuia rosea

Genus image · Cirad · Public domain
Range not recordedhardwood1,054 lbf*39.6 lb/ft³*
Pipli

Bucklandia populnea

Asiahardwood1,145 lbf40.0 lb/ft³
Piquia

Caryocar spp.

Genus image · Cirad · Public domain
Tropical Americahardwood1,720 lbf54.0 lb/ft³
Pitch pine

Pinus rigida

Genus image · Cirad · Public domain
North Americasoftwood717 lbf*36.3 lb/ft³
Range not recordedhardwood1,054 lbf*39.6 lb/ft³*
Pochote

Bombacopsis quinata

Genus image · Cirad · Public domain
Tropical Americahardwood720 lbf33.9 lb/ft³*
Pochote

Ceiba aesculifolia

Genus image · Cirad · Public domain
Range not recordedhardwood641 lbf*31.5 lb/ft³*
Podo

Podocarpus spp.

Genus image · Cirad · Public domain
Africasoftwood830 lbf32.0 lb/ft³
Podocarp

Podocarpus spp.

Genus image · Cirad · Public domain
Tropical Americasoftwood760 lbf35.0 lb/ft³
Poinsettia

Euphorbia pulcherrima

Frank Vincentz · CC BY-SA 3.0
Range not recordedhardwood714 lbf*33.1 lb/ft³*
Poison ash

Comocladia dodonaea

Xemenendura · CC BY-SA 3.0
Range not recordedhardwood3,749 lbf*71.5 lb/ft³*
Poison devil's-pepper

Rauvolfia vomitoria

Genus image · Cirad · Public domain
Range not recordedhardwood1,007 lbf*38.8 lb/ft³*
Poison sumac

Toxicodendron vernix

Genus image · Cirad · Public domain
Range not recordedhardwood714 lbf*33.1 lb/ft³*
Range not recordedhardwood1,990 lbf*53.3 lb/ft³*
Pond pine

Pinus serotina

Genus image · Cirad · Public domain
North Americasoftwood803 lbf*39.1 lb/ft³
Pond-apple

Annona glabra

Genus image · Cirad · Public domain
Range not recordedhardwood753 lbf*33.9 lb/ft³*
Pondcypress

Taxodium ascendens

Wikidata via Wikimedia Commons · Public domain
Range not recordedsoftwood576 lbf*31.5 lb/ft³*
North Americasoftwood460 lbf28.0 lb/ft³
Port Jackson fig

Ficus rubiginosa

Genus image · Cirad · Public domain
Range not recordedhardwood679 lbf*32.3 lb/ft³*
North Americasoftwood630 lbf30.1 lb/ft³
Portia tree

Thespesia populnea

Cirad · Public domain
Range not recordedhardwood1,103 lbf*40.5 lb/ft³*
Post oak

Quercus stellata

Genus image · Cirad · Public domain
North Americahardwood1,360 lbf46.8 lb/ft³
Potatotree

Solanum erianthum

Genus image · Cirad · Public domain
Range not recordedhardwood679 lbf*32.3 lb/ft³*
Poumuli

Flueggea flexuosa

Greg III Espera · CC BY
Range not recordedhardwood2,064 lbf*54.2 lb/ft³*
Pracuúba-da-terra-firme

Trichilia lecointei

Genus image · Cirad · Public domain
Tropical Americahardwood3,159 lbf73.4 lb/ft³*
Prairie crab apple

Malus ioensis

Genus image · Denisjchevalier · CC BY-SA 4.0
Range not recordedhardwood1,538 lbf*47.3 lb/ft³*
Prairie sumac

Rhus lanceolata

Genus image · Cirad · Public domain
Range not recordedhardwood679 lbf*32.3 lb/ft³*
Range not recordedhardwood395 lbf*25.1 lb/ft³*
Prickly Moses

Acacia verticillata

Genus image · Cirad · Public domain
Range not recordedhardwood1,054 lbf*39.6 lb/ft³*
Prickly yellow

Zanthoxylum caribaeum

Cirad · Public domain
Range not recordedhardwood1,923 lbf*52.4 lb/ft³*
Pride of India

Lagerstroemia speciosa

Genus image · Cirad · Public domain
Range not recordedhardwood1,203 lbf*42.1 lb/ft³*
Pride-of-Barbados

Caesalpinia pulcherrima

Genus image · Cirad · Public domain
Range not recordedhardwood1,598 lbf*48.1 lb/ft³*
Primavera

Tabebuia donnell–smithii

Genus image · Cirad · Public domain
Tropical Americahardwood660 lbf29.0 lb/ft³
Asiahardwood1,300 lbf41.0 lb/ft³
Privet stopper

Eugenia ligustrina

Genus image · Cirad · Public domain
Range not recordedhardwood2,692 lbf*61.3 lb/ft³*
Pterygota

Pterygota spp.

Genus image · Cirad · Public domain
Africahardwood955 lbf39.0 lb/ft³
Pua, Chinese lantern tree

Hernandia nymphaeifolia

Cirad · Public domain
Range not recordedhardwood344 lbf*23.5 lb/ft³*
Pualulu

Fagraea berteroana

Cirad · Public domain
Range not recordedhardwood1,658 lbf*48.9 lb/ft³*
Puapua

Guettarda speciosa

Cirad · Public domain
Range not recordedhardwood1,152 lbf*41.3 lb/ft³*
Range not recordedhardwood1,255 lbf*43.0 lb/ft³*
Puerto Rico bully

Sideroxylon portoricense

Genus image · Cirad · Public domain
Range not recordedhardwood2,692 lbf*61.3 lb/ft³*
Puerto Rico cinnamon

Licaria parvifolia

Genus image · Cirad · Public domain
Range not recordedhardwood2,367 lbf*57.7 lb/ft³*
Puerto Rico holly

Ilex nitida

Genus image · Cirad · Public domain
Range not recordedhardwood2,139 lbf*55.1 lb/ft³*
Puerto Rico magnolia

Magnolia portoricensis

Genus image · Cirad · Public domain
Range not recordedhardwood1,203 lbf*42.1 lb/ft³*
Puerto Rico royal palm

Roystonea borinquena

wisel · CC BY 4.0
Range not recordedhardwood2,287 lbf*56.9 lb/ft³*
Pulai

Alstonia spp.

Genus image · Cirad · Public domain
Oceaniahardwood460 lbf28.0 lb/ft³
Pulasan

Nephelium ramboutan-ake

Genus image · Cirad · Public domain
Range not recordedhardwood2,692 lbf*61.3 lb/ft³*
Pulu

Tabernaemontana pandacaqui

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Pumpkin ash

Fraxinus profunda

Genus image · Cirad · Public domain
North Americahardwood875 lbf*36.3 lb/ft³*
Pumpwood

Cecropia schreberiana

Genus image · Cirad · Public domain
Range not recordedhardwood298 lbf*22.0 lb/ft³*
Punah

Tetramerista glabra

Cirad · Public domain
Asiahardwood910 lbf45.0 lb/ft³
Punchberry

Myrcia splendens

Cirad · Public domain
Range not recordedhardwood2,210 lbf*55.9 lb/ft³*
Pungent oak

Quercus pungens

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Purple blow maple

Acer truncatum

Genus image · Cirad · Public domain
Range not recordedhardwood832 lbf*35.5 lb/ft³*
Purple mombin

Spondias purpurea

Genus image · Cirad · Public domain
Range not recordedhardwood423 lbf*26.0 lb/ft³*