All wood species
1,785 species. 571 carry a published Janka test. A species with no test says so.
1,785 matching species · Estimates are marked with an asterisk. Images may show a related species; see credits.
| Wood | Region | Wood type | Janka hardness | Density |
|---|---|---|---|---|
Samoensis Citronella samoensis | Range not recorded | hardwood | 1,725 lbf* | 49.9 lb/ft³* |
| Tropical America | hardwood | 2,692 lbf* | 59.0 lb/ft³ | |
| Range not recorded | hardwood | 1,598 lbf* | 48.1 lb/ft³* | |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| North America | softwood | 635 lbf* | 33.6 lb/ft³ | |
| Oceania | hardwood | 1,680 lbf | 58.0 lb/ft³ | |
| Tropical America | hardwood | 900 lbf | 37.1 lb/ft³* | |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| Range not recorded | softwood | 449 lbf* | 26.7 lb/ft³* | |
| Tropical America | hardwood | 1,150 lbf | 39.0 lb/ft³ | |
| Range not recorded | hardwood | 714 lbf* | 33.1 lb/ft³* | |
| Africa | hardwood | 1,510 lbf | 42.0 lb/ft³ | |
| Africa | hardwood | 1,103 lbf* | 41.0 lb/ft³ | |
| Range not recorded | hardwood | 3,054 lbf* | 65.0 lb/ft³* | |
| Tropical America | hardwood | 3,100 lbf | 58.0 lb/ft³ | |
| Tropical America | hardwood | 2,831 lbf | 67.7 lb/ft³* | |
| Range not recorded | hardwood | 1,475 lbf* | 46.4 lb/ft³* | |
| Range not recorded | hardwood | 832 lbf* | 35.5 lb/ft³* | |
| North America | hardwood | 672 lbf* | 32.2 lb/ft³ | |
| Range not recorded | hardwood | 2,607 lbf* | 60.4 lb/ft³* | |
Sawara-cypress Chamaecyparis pisifera Original: Raita Futo from Tokyo, Japan; this edit: User:MPF · CC BY 2.0 | Range not recorded | softwood | 469 lbf* | 27.5 lb/ft³* |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| Range not recorded | hardwood | 1,788 lbf* | 50.7 lb/ft³* | |
| North America | hardwood | 1,400 lbf | 46.8 lb/ft³ | |
| Range not recorded | hardwood | 641 lbf* | 31.5 lb/ft³* | |
| Range not recorded | hardwood | 1,538 lbf* | 47.3 lb/ft³* | |
| Europe | softwood | 621 lbf* | 33.1 lb/ft³* | |
| Range not recorded | hardwood | 451 lbf* | 26.7 lb/ft³* | |
| Range not recorded | hardwood | 197 lbf* | 18.2 lb/ft³* | |
| Range not recorded | hardwood | 2,779 lbf* | 62.2 lb/ft³* | |
| Range not recorded | hardwood | 1,598 lbf* | 48.1 lb/ft³* | |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| Range not recorded | hardwood | 1,852 lbf* | 51.5 lb/ft³* | |
| Range not recorded | hardwood | 1,054 lbf* | 39.6 lb/ft³* | |
| Range not recorded | hardwood | 608 lbf* | 30.7 lb/ft³* | |
| Range not recorded | hardwood | 3,749 lbf* | 71.5 lb/ft³* | |
| Range not recorded | hardwood | 2,064 lbf* | 54.2 lb/ft³* | |
| Range not recorded | hardwood | 1,725 lbf* | 49.9 lb/ft³* | |
| Range not recorded | hardwood | 1,309 lbf* | 43.8 lb/ft³* | |
| Asia | hardwood | 1,410 lbf | 42.0 lb/ft³ | |
| Range not recorded | hardwood | 1,152 lbf* | 41.3 lb/ft³* | |
| Range not recorded | softwood | 449 lbf* | 26.7 lb/ft³* | |
Seringarana Micrandra rossiana | Tropical America | hardwood | 1,925 lbf | 50.6 lb/ft³ |
| Tropical America | hardwood | 1,538 lbf* | 46.0 lb/ft³ | |
| Range not recorded | hardwood | 1,788 lbf* | 50.7 lb/ft³* | |
| Tropical America | hardwood | 1,153 lbf | 46.8 lb/ft³ | |
| North America | hardwood | 1,880 lbf | 50.3 lb/ft³ | |
| Range not recorded | hardwood | 1,203 lbf* | 42.1 lb/ft³* | |
| Range not recorded | softwood | 449 lbf* | 26.7 lb/ft³* | |
| North America | hardwood | 1,810 lbf | 48.3 lb/ft³ | |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| Range not recorded | hardwood | 679 lbf* | 32.3 lb/ft³* | |
Shirakiopsis indica Shirakiopsis indica | Range not recorded | hardwood | 915 lbf* | 37.1 lb/ft³* |
| Range not recorded | hardwood | 451 lbf* | 26.7 lb/ft³* | |
| Asia | hardwood | 1,780 lbf | 53.3 lb/ft³* | |
| North America | softwood | 690 lbf | 35.6 lb/ft³ | |
| Range not recorded | hardwood | 753 lbf* | 33.9 lb/ft³* | |
| Range not recorded | hardwood | 1,203 lbf* | 42.1 lb/ft³* | |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| Range not recorded | hardwood | 1,990 lbf* | 53.3 lb/ft³* | |
| Asia | hardwood | 3,441 lbf* | 68.7 lb/ft³* | |
| Range not recorded | hardwood | 1,538 lbf* | 47.3 lb/ft³* | |
| Range not recorded | hardwood | 1,152 lbf* | 41.3 lb/ft³* | |
| Range not recorded | hardwood | 1,538 lbf* | 47.3 lb/ft³* | |
Silk cottontree Cochlospermum vitifolium | Range not recorded | hardwood | 149 lbf* | 15.9 lb/ft³* |
| Range not recorded | hardwood | 573 lbf* | 29.8 lb/ft³* | |
| Range not recorded | hardwood | 451 lbf* | 26.7 lb/ft³* | |
| Oceania | hardwood | 840 lbf | 38.0 lb/ft³ | |
| Europe | hardwood | 1,203 lbf* | 42.1 lb/ft³* | |
| Range not recorded | hardwood | 1,363 lbf* | 44.7 lb/ft³* | |
| Europe | softwood | 576 lbf* | 31.5 lb/ft³* | |
| Range not recorded | hardwood | 344 lbf* | 23.5 lb/ft³* | |
| North America | hardwood | 700 lbf | 32.8 lb/ft³ | |
| Range not recorded | hardwood | 423 lbf* | 26.0 lb/ft³* | |
| Range not recorded | hardwood | 1,054 lbf* | 39.6 lb/ft³* | |
| Range not recorded | hardwood | 1,054 lbf* | 39.6 lb/ft³* | |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| Range not recorded | hardwood | 1,309 lbf* | 43.8 lb/ft³* | |
| Asia | hardwood | 1,250 lbf | 45.0 lb/ft³ | |
| Range not recorded | hardwood | 753 lbf* | 33.9 lb/ft³* | |
| Range not recorded | softwood | 599 lbf* | 32.3 lb/ft³* | |
| North America | softwood | 510 lbf | 28.0 lb/ft³ | |
| Range not recorded | hardwood | 451 lbf* | 26.7 lb/ft³* | |
| North America | softwood | 869 lbf* | 41.3 lb/ft³ | |
| North America | hardwood | 860 lbf | 37.1 lb/ft³ | |
| Range not recorded | hardwood | 1,255 lbf* | 43.0 lb/ft³* | |
| Range not recorded | hardwood | 2,367 lbf* | 57.7 lb/ft³* | |
| Range not recorded | hardwood | 2,692 lbf* | 61.3 lb/ft³* | |
| Range not recorded | hardwood | 2,139 lbf* | 55.1 lb/ft³* | |
| Range not recorded | hardwood | 451 lbf* | 26.7 lb/ft³* | |
| Range not recorded | hardwood | 1,054 lbf* | 39.6 lb/ft³* | |
| Range not recorded | hardwood | 1,309 lbf* | 43.8 lb/ft³* | |
| Range not recorded | hardwood | 451 lbf* | 26.7 lb/ft³* | |
| Range not recorded | hardwood | 2,367 lbf* | 57.7 lb/ft³* | |
| Range not recorded | hardwood | 714 lbf* | 33.1 lb/ft³* | |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| Range not recorded | hardwood | 753 lbf* | 33.9 lb/ft³* | |
| Africa | hardwood | 875 lbf* | 36.0 lb/ft³ | |
Sorva Malouetia duckei | Tropical America | hardwood | 1,329 lbf | 43.8 lb/ft³* |
| Range not recorded | hardwood | 832 lbf* | 35.5 lb/ft³* |