All wood species
1,785 species. 571 carry a published Janka test. A species with no test says so.
1,785 matching species · Estimates are marked with an asterisk. Images may show a related species; see credits.
| Wood | Region | Wood type | Janka hardness | Density |
|---|---|---|---|---|
| Tropical America | hardwood | 1,479 lbf | 50.7 lb/ft³* | |
| Tropical America | hardwood | 1,962 lbf | 47.3 lb/ft³* | |
| Tropical America | hardwood | 1,166 lbf | 40.0 lb/ft³ | |
| Africa | hardwood | 1,250 lbf | 40.0 lb/ft³ | |
| Range not recorded | hardwood | 915 lbf* | 37.1 lb/ft³* | |
| Range not recorded | hardwood | 2,064 lbf* | 54.2 lb/ft³* | |
| Asia | hardwood | 1,000 lbf | 40.0 lb/ft³ | |
| Asia | hardwood | 2,120 lbf | 56.0 lb/ft³ | |
| Range not recorded | hardwood | 1,007 lbf* | 38.8 lb/ft³* | |
| Tropical America | hardwood | 1,688 lbf | 45.6 lb/ft³ | |
| Tropical America | hardwood | 1,378 lbf | 44.9 lb/ft³ | |
| Range not recorded | hardwood | 3,147 lbf* | 65.9 lb/ft³* | |
| Range not recorded | hardwood | 1,007 lbf* | 38.8 lb/ft³* | |
| Range not recorded | hardwood | 1,475 lbf* | 46.4 lb/ft³* | |
| Range not recorded | hardwood | 1,363 lbf* | 44.7 lb/ft³* | |
| Range not recorded | hardwood | 1,598 lbf* | 48.1 lb/ft³* | |
| Range not recorded | hardwood | 1,725 lbf* | 49.9 lb/ft³* | |
| Range not recorded | hardwood | 1,725 lbf* | 49.9 lb/ft³* | |
| Range not recorded | hardwood | 714 lbf* | 33.1 lb/ft³* | |
| Range not recorded | hardwood | 2,058 lbf* | 54.1 lb/ft³* | |
| Asia | hardwood | 1,255 lbf | 48.0 lb/ft³ | |
| Asia | hardwood | 1,118 lbf | 40.0 lb/ft³ | |
Thitpok Tetrameies nudiflora | Asia | hardwood | 298 lbf* | 22.0 lb/ft³ |
| Range not recorded | hardwood | 832 lbf* | 35.5 lb/ft³* | |
| Range not recorded | hardwood | 2,287 lbf* | 56.9 lb/ft³* | |
| Range not recorded | hardwood | 197 lbf* | 18.2 lb/ft³* | |
| Tropical America | hardwood | 1,537 lbf | 34.3 lb/ft³ | |
| Range not recorded | hardwood | 1,363 lbf* | 44.7 lb/ft³* | |
| Range not recorded | hardwood | 321 lbf* | 22.8 lb/ft³* | |
| Range not recorded | hardwood | 960 lbf* | 38.0 lb/ft³* | |
| Range not recorded | hardwood | 641 lbf* | 31.5 lb/ft³* | |
| Oceania | hardwood | 550 lbf | 31.5 lb/ft³* | |
| Tropical America | hardwood | 787 lbf | 35.0 lb/ft³ | |
| Range not recorded | softwood | 599 lbf* | 32.3 lb/ft³* | |
| Oceania | softwood | 655 lbf | 32.0 lb/ft³ | |
| Range not recorded | hardwood | 509 lbf* | 28.2 lb/ft³* | |
| Range not recorded | hardwood | 1,054 lbf* | 39.6 lb/ft³* | |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| Range not recorded | hardwood | 1,923 lbf* | 52.4 lb/ft³* | |
| Range not recorded | hardwood | 134 lbf* | 15.2 lb/ft³* | |
| Range not recorded | hardwood | 197 lbf* | 18.2 lb/ft³* | |
| Range not recorded | hardwood | 641 lbf* | 31.5 lb/ft³* | |
Trichospermum ikutai Trichospermum ikutai | Range not recorded | hardwood | 423 lbf* | 26.0 lb/ft³* |
| Range not recorded | hardwood | 832 lbf* | 35.5 lb/ft³* | |
| Range not recorded | hardwood | 1,152 lbf* | 41.3 lb/ft³* | |
| Tropical America | hardwood | 800 lbf | 41.0 lb/ft³ | |
| Range not recorded | hardwood | 321 lbf* | 22.8 lb/ft³* | |
| Tropical America | hardwood | 320 lbf | 23.0 lb/ft³ | |
| Range not recorded | hardwood | 2,530 lbf* | 59.6 lb/ft³* | |
| Range not recorded | hardwood | 479 lbf* | 27.5 lb/ft³* | |
| Range not recorded | hardwood | 542 lbf* | 29.1 lb/ft³* | |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| Range not recorded | hardwood | 1,203 lbf* | 42.1 lb/ft³* | |
| Oceania | hardwood | 2,750 lbf | 60.0 lb/ft³ | |
| Tropical America | hardwood | 2,396 lbf | 56.9 lb/ft³* | |
| Tropical America | hardwood | 2,923 lbf | 59.9 lb/ft³ | |
| Range not recorded | hardwood | 2,607 lbf* | 60.4 lb/ft³* | |
| Range not recorded | hardwood | 641 lbf* | 31.5 lb/ft³* | |
| Tropical America | hardwood | 496 lbf | 35.5 lb/ft³* | |
| Tropical America | hardwood | 817 lbf | 36.8 lb/ft³ | |
| Tropical America | hardwood | 1,195 lbf | 48.9 lb/ft³* | |
| Range not recorded | hardwood | 2,367 lbf* | 57.7 lb/ft³* | |
| Range not recorded | hardwood | 1,103 lbf* | 40.5 lb/ft³* | |
| Tropical America | hardwood | 875 lbf* | 38.0 lb/ft³ | |
| Range not recorded | hardwood | 276 lbf* | 21.2 lb/ft³* | |
| Range not recorded | hardwood | 679 lbf* | 32.3 lb/ft³* | |
| Asia | hardwood | 3,147 lbf* | 63.0 lb/ft³ | |
Urucu-da-mata Bixa arborea | Tropical America | hardwood | 437 lbf | 23.5 lb/ft³* |
| Tropical America | hardwood | 4,057 lbf | 67.4 lb/ft³ | |
| Tropical America | hardwood | 4,206 lbf | 59.9 lb/ft³ | |
| Tropical America | hardwood | 2,469 lbf | 57.4 lb/ft³ | |
| Range not recorded | softwood | 1,282 lbf* | 53.3 lb/ft³* | |
| Africa | hardwood | 1,260 lbf | 41.0 lb/ft³ | |
| Range not recorded | hardwood | 1,255 lbf* | 43.0 lb/ft³* | |
| Tropical America | hardwood | 2,335 lbf | 62.2 lb/ft³* | |
| Tropical America | hardwood | 2,948 lbf | 69.7 lb/ft³* | |
| Range not recorded | hardwood | 1,852 lbf* | 51.5 lb/ft³* | |
| Range not recorded | hardwood | 1,007 lbf* | 38.8 lb/ft³* | |
| Range not recorded | hardwood | 1,852 lbf* | 51.5 lb/ft³* | |
| Range not recorded | hardwood | 608 lbf* | 30.7 lb/ft³* | |
| Range not recorded | hardwood | 1,007 lbf* | 38.8 lb/ft³* | |
| Range not recorded | hardwood | 2,779 lbf* | 62.2 lb/ft³* | |
| Range not recorded | hardwood | 1,103 lbf* | 40.5 lb/ft³* | |
| Tropical America | hardwood | 5,180 lbf* | 78.0 lb/ft³ | |
| Range not recorded | hardwood | 276 lbf* | 21.2 lb/ft³* | |
| Range not recorded | hardwood | 832 lbf* | 35.5 lb/ft³* | |
| Range not recorded | hardwood | 2,139 lbf* | 55.1 lb/ft³* | |
| North America | softwood | 740 lbf | 33.6 lb/ft³ | |
| Range not recorded | hardwood | 1,007 lbf* | 38.8 lb/ft³* | |
| Tropical America | hardwood | 1,041 lbf | 38.0 lb/ft³* | |
| Tropical America | hardwood | 624 lbf | 28.7 lb/ft³ | |
| Africa | hardwood | 680 lbf | 29.8 lb/ft³* | |
| Range not recorded | hardwood | 1,203 lbf* | 42.1 lb/ft³* | |
| Tropical America | hardwood | 2,867 lbf* | 59.0 lb/ft³ | |
| Range not recorded | hardwood | 369 lbf* | 24.3 lb/ft³* | |
| Tropical America | hardwood | 2,040 lbf | 58.0 lb/ft³ | |
| Tropical America | hardwood | 3,692 lbf | 70.0 lb/ft³ | |
| Range not recorded | hardwood | 1,658 lbf* | 48.9 lb/ft³* | |
| Range not recorded | softwood | 599 lbf* | 32.3 lb/ft³* | |
| Range not recorded | hardwood | 1,007 lbf* | 38.8 lb/ft³* |