All wood species
1,785 species. 571 carry a published Janka test. A species with no test says so.
1,785 matching species · Estimates are marked with an asterisk. Images may show a related species; see credits.
| Wood | Region | Wood type | Janka hardness | Density |
|---|---|---|---|---|
| Africa | hardwood | 2,287 lbf* | 55.0 lb/ft³ | |
| Africa | hardwood | 995 lbf | 33.0 lb/ft³ | |
| Range not recorded | hardwood | 1,255 lbf* | 43.0 lb/ft³* | |
Anoerá-ferro Acioa sp | Tropical America | hardwood | 2,683 lbf | 60.6 lb/ft³ |
| Range not recorded | hardwood | 960 lbf* | 38.0 lb/ft³* | |
| Africa | hardwood | 500 lbf | 27.0 lb/ft³ | |
| Range not recorded | hardwood | 1,475 lbf* | 46.4 lb/ft³* | |
| Range not recorded | hardwood | 791 lbf* | 34.7 lb/ft³* | |
| Range not recorded | hardwood | 423 lbf* | 26.0 lb/ft³* | |
| Range not recorded | softwood | 599 lbf* | 32.3 lb/ft³* | |
| Europe | hardwood | 1,658 lbf* | 48.9 lb/ft³* | |
| Range not recorded | hardwood | 1,725 lbf* | 49.9 lb/ft³* | |
| Range not recorded | hardwood | 2,367 lbf* | 57.7 lb/ft³* | |
| Range not recorded | hardwood | 1,725 lbf* | 49.9 lb/ft³* | |
| Range not recorded | hardwood | 1,598 lbf* | 48.1 lb/ft³* | |
| Tropical America | hardwood | 1,153 lbf | 39.3 lb/ft³ | |
| Tropical America | hardwood | 1,757 lbf | 51.2 lb/ft³ | |
| Tropical America | hardwood | 1,208 lbf | 40.0 lb/ft³ | |
Arariba Centrolobium spp. | Tropical America | hardwood | 1,030 lbf | 50.0 lb/ft³ |
Araríba Sickingia spp. | Tropical America | hardwood | 1,054 lbf* | 40.0 lb/ft³ |
| Range not recorded | hardwood | 1,309 lbf* | 43.8 lb/ft³* | |
| Range not recorded | hardwood | 2,210 lbf* | 55.9 lb/ft³* | |
| Range not recorded | hardwood | 479 lbf* | 27.5 lb/ft³* | |
| Range not recorded | hardwood | 1,363 lbf* | 44.7 lb/ft³* | |
| Range not recorded | softwood | 599 lbf* | 32.3 lb/ft³* | |
| Range not recorded | hardwood | 791 lbf* | 34.7 lb/ft³* | |
| Range not recorded | hardwood | 714 lbf* | 33.1 lb/ft³* | |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| Tropical America | hardwood | 2,960 lbf | 72.0 lb/ft³* | |
| Range not recorded | hardwood | 791 lbf* | 34.7 lb/ft³* | |
| Range not recorded | hardwood | 875 lbf* | 36.3 lb/ft³* | |
| Range not recorded | softwood | 645 lbf* | 33.9 lb/ft³* | |
| Range not recorded | hardwood | 2,367 lbf* | 57.7 lb/ft³* | |
| Range not recorded | hardwood | 1,007 lbf* | 38.8 lb/ft³* | |
| Range not recorded | hardwood | 1,255 lbf* | 43.0 lb/ft³* | |
Atlantic white cedar Chamaecyparis thyoides Robert H. Mohlenbrock @ USDA-NRCS PLANTS Database / USDA NRCS. 1995. Northeast w · Public domain | North America | softwood | 350 lbf | 22.3 lb/ft³ |
| Range not recorded | softwood | 554 lbf* | 30.7 lb/ft³* | |
| Range not recorded | hardwood | 1,725 lbf* | 49.9 lb/ft³* | |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| Range not recorded | hardwood | 1,598 lbf* | 48.1 lb/ft³* | |
| Oceania | hardwood | 1,100 lbf | 40.0 lb/ft³ | |
| Range not recorded | hardwood | 1,788 lbf* | 50.7 lb/ft³* | |
| Range not recorded | hardwood | 641 lbf* | 31.5 lb/ft³* | |
| Range not recorded | hardwood | 3,054 lbf* | 65.0 lb/ft³* | |
| Range not recorded | softwood | 599 lbf* | 32.3 lb/ft³* | |
| Range not recorded | hardwood | 1,658 lbf* | 48.9 lb/ft³* | |
| Range not recorded | hardwood | 791 lbf* | 34.7 lb/ft³* | |
| Africa | hardwood | 1,080 lbf | 36.0 lb/ft³ | |
| Tropical America | hardwood | 686 lbf | 38.1 lb/ft³ | |
| Africa | hardwood | 1,230 lbf | 45.0 lb/ft³ | |
| Africa | hardwood | 3,350 lbf | 70.0 lb/ft³ | |
Azulejo Cornutia pyramidata | Range not recorded | hardwood | 2,064 lbf* | 54.2 lb/ft³* |
| Range not recorded | hardwood | 1,923 lbf* | 52.4 lb/ft³* | |
| North America | softwood | 510 lbf | 32.2 lb/ft³ | |
| Tropical America | hardwood | 88 lbf | 11.5 lb/ft³* | |
| North America | softwood | 380 lbf | 24.5 lb/ft³ | |
Balsam poplar Populus balsamifera Lynden Gerdes @ USDA-NRCS PLANTS Database / USDA NRCS. 1995. Northeast wetland f · Public domain | North America | hardwood | 351 lbf* | 23.8 lb/ft³ |
| Range not recorded | hardwood | 451 lbf* | 26.7 lb/ft³* | |
| Tropical America | hardwood | 2,200 lbf | 58.0 lb/ft³ | |
| Tropical America | hardwood | 510 lbf | 36.0 lb/ft³ | |
| Range not recorded | hardwood | 2,530 lbf* | 59.6 lb/ft³* | |
| Asia | hardwood | 1,309 lbf* | 44.0 lb/ft³ | |
| Range not recorded | hardwood | 321 lbf* | 22.8 lb/ft³* | |
| Tropical America | hardwood | 1,000 lbf | 44.0 lb/ft³ | |
| Range not recorded | hardwood | 181 lbf* | 17.5 lb/ft³* | |
| Tropical America | hardwood | 720 lbf | 41.0 lb/ft³ | |
| Tropical America | hardwood | 2,693 lbf | 57.4 lb/ft³ | |
| Range not recorded | hardwood | 1,725 lbf* | 49.9 lb/ft³* | |
| Range not recorded | hardwood | 1,203 lbf* | 42.1 lb/ft³* | |
| Range not recorded | hardwood | 1,852 lbf* | 51.5 lb/ft³* | |
| Range not recorded | hardwood | 1,475 lbf* | 46.4 lb/ft³* | |
| Range not recorded | hardwood | 2,692 lbf* | 61.3 lb/ft³* | |
| Range not recorded | hardwood | 1,658 lbf* | 48.9 lb/ft³* | |
| Range not recorded | hardwood | 2,210 lbf* | 55.9 lb/ft³* | |
| Range not recorded | hardwood | 1,007 lbf* | 38.8 lb/ft³* | |
| Asia | hardwood | 344 lbf* | 24.0 lb/ft³ | |
| Range not recorded | hardwood | 2,367 lbf* | 57.7 lb/ft³* | |
| Range not recorded | hardwood | 2,867 lbf* | 63.1 lb/ft³* | |
| Range not recorded | hardwood | 3,147 lbf* | 65.9 lb/ft³* | |
| Range not recorded | hardwood | 3,241 lbf* | 66.9 lb/ft³* | |
| Range not recorded | hardwood | 451 lbf* | 26.7 lb/ft³* | |
| Range not recorded | hardwood | 875 lbf* | 36.3 lb/ft³* | |
| Asia | hardwood | 3,020 lbf | 68.0 lb/ft³ | |
| Africa | hardwood | 1,750 lbf | 50.0 lb/ft³ | |
| Asia | softwood | 605 lbf | 35.0 lb/ft³ | |
| Asia | hardwood | 960 lbf* | 42.0 lb/ft³ | |
| Range not recorded | hardwood | 1,007 lbf* | 38.8 lb/ft³* | |
| Africa | hardwood | 1,360 lbf | 44.7 lb/ft³* | |
| Range not recorded | softwood | 792 lbf* | 38.8 lb/ft³* | |
| Range not recorded | hardwood | 875 lbf* | 36.3 lb/ft³* | |
| Range not recorded | softwood | 645 lbf* | 33.9 lb/ft³* | |
| Range not recorded | hardwood | 679 lbf* | 32.3 lb/ft³* | |
| North America | hardwood | 850 lbf | 33.6 lb/ft³ | |
| North America | hardwood | 471 lbf* | 27.3 lb/ft³ | |
| Range not recorded | hardwood | 832 lbf* | 35.5 lb/ft³* | |
| Range not recorded | hardwood | 875 lbf* | 36.3 lb/ft³* | |
| Asia | hardwood | 1,475 lbf | 40.0 lb/ft³ | |
| Asia | hardwood | 362 lbf | 23.0 lb/ft³ | |
| Range not recorded | hardwood | 2,779 lbf* | 62.2 lb/ft³* |