Wood Record

All wood species

1,785 species. 571 carry a published Janka test. A species with no test says so.

1,785 matching species · Estimates are marked with an asterisk. Images may show a related species; see credits.

Wood species and selected properties
WoodRegionWood typeJanka hardnessDensity
Fava-orelha-de-negro

Enterolobium schomburgkii

Cirad · Public domain
Tropical Americahardwood2,346 lbf62.0 lb/ft³
Faveira

Parkia nitida = Parkia oppositifolia

Cirad · Public domain
Tropical Americahardwood621 lbf27.5 lb/ft³
Faveira

Parkia multijuga

Cirad · Public domain
Tropical Americahardwood668 lbf28.2 lb/ft³*
Faveira / visgueiro

Parkia paraensis

Genus image · Cirad · Public domain
Tropical Americahardwood743 lbf33.1 lb/ft³*
Faveira-amargosa

Vatairea paraensis

Cirad · Public domain
Tropical Americahardwood2,174 lbf62.2 lb/ft³*
Faveira-amargosa

Vatairea guianensis

Cirad · Public domain
Tropical Americahardwood1,532 lbf51.8 lb/ft³
Faveira-amargosa

Vataireopsis speciosa

Cirad · Public domain
Tropical Americahardwood1,043 lbf46.2 lb/ft³
Range not recordedhardwood1,788 lbf*50.7 lb/ft³*
Ferntree

Filicium decipiens

Cirad · Public domain
Range not recordedhardwood1,990 lbf*53.3 lb/ft³*
Ficus copiosa

Ficus copiosa

Genus image · Cirad · Public domain
Range not recordedhardwood915 lbf*37.1 lb/ft³*
Ficus lutea

Ficus lutea

Genus image · Cirad · Public domain
Range not recordedhardwood479 lbf*27.5 lb/ft³*
Fiddlewood

Vitex spp.

Genus image · Cirad · Public domain
Tropical Americahardwood1,160 lbf43.0 lb/ft³
Figueira / gameleira

Ficus insipida

Genus image · Cirad · Public domain
Tropical Americahardwood269 lbf28.1 lb/ft³
Range not recordedhardwood2,530 lbf*59.6 lb/ft³*
Range not recordedhardwood1,990 lbf*53.3 lb/ft³*
Five-needle pine

Pinus parviflora

Genus image · Cirad · Public domain
Range not recordedsoftwood599 lbf*32.3 lb/ft³*
Range not recordedhardwood1,054 lbf*39.6 lb/ft³*
Range not recordedhardwood369 lbf*24.3 lb/ft³*
Flor de San Jose

Senna atomaria

Genus image · Cirad · Public domain
Range not recordedhardwood1,658 lbf*48.9 lb/ft³*
Range not recordedhardwood1,852 lbf*51.5 lb/ft³*
Range not recordedhardwood1,852 lbf*51.5 lb/ft³*
Florida hopbush

Dodonaea viscosa

Cirad · Public domain
Range not recordedhardwood3,336 lbf*67.7 lb/ft³*
Florida maple

Acer barbatum

Genus image · Cirad · Public domain
Range not recordedhardwood832 lbf*35.5 lb/ft³*
Range not recordedhardwood915 lbf*37.1 lb/ft³*
Florida strangler fig

Ficus aurea

Genus image · Cirad · Public domain
Range not recordedhardwood753 lbf*33.9 lb/ft³*
Range not recordedsoftwood645 lbf*33.9 lb/ft³*
Florida yew

Taxus floridana

Genus image · Cirad · Public domain
Range not recordedsoftwood1,038 lbf*46.4 lb/ft³*
Range not recordedhardwood1,203 lbf*42.1 lb/ft³*
Range not recordedhardwood1,725 lbf*49.9 lb/ft³*
Forest nightshade

Solanum nudum

Genus image · Cirad · Public domain
Range not recordedhardwood753 lbf*33.9 lb/ft³*
Forest redgum

Eucalyptus tereticornis

Genus image · Cirad · Public domain
Range not recordedhardwood2,367 lbf*57.7 lb/ft³*
Range not recordedhardwood216 lbf*19.0 lb/ft³*
Four-leaf or Parry pinyon pine

Pinus quadrifolia

Genus image · Cirad · Public domain
Range not recordedsoftwood599 lbf*32.3 lb/ft³*
Foxtail pine

Pinus balfouriana

Genus image · Cirad · Public domain
Range not recordedsoftwood599 lbf*32.3 lb/ft³*
Range not recordedhardwood679 lbf*32.3 lb/ft³*
Fragrant manjack

Cordia dichotoma

Genus image · Cirad · Public domain
Range not recordedhardwood451 lbf*26.7 lb/ft³*
Fraser fir

Abies fraseri

Genus image · Cirad · Public domain
Range not recordedsoftwood449 lbf*26.7 lb/ft³*
Fraser magnolia

Magnolia fraseri

Genus image · Cirad · Public domain
Range not recordedhardwood573 lbf*29.8 lb/ft³*
Frei-jorge

Cordia sp.

Genus image · Cirad · Public domain
Tropical Americahardwood960 lbf*40.0 lb/ft³
Freijó

Cordia bicolor

Genus image · Cirad · Public domain
Tropical Americahardwood963 lbf37.1 lb/ft³*
Freijó

Cordia goeldiana

Cirad · Public domain
Tropical Americahardwood996 lbf36.3 lb/ft³*
Freijó

Cordia sagotii

Cirad · Public domain
Tropical Americahardwood882 lbf38.0 lb/ft³*
Fremont cottonwood

Populus fremontii

Amy Gaiennie, NPS · Public domain
Range not recordedhardwood608 lbf*30.7 lb/ft³*
Fustic

Chlorophora tinctoria

Cirad · Public domain
Tropical Americahardwood2,380 lbf56.0 lb/ft³
Fustic

Pictetia aculeata

Daniel Cahen · CC BY
Range not recordedhardwood2,139 lbf*55.1 lb/ft³*
Gaita

Trichilia pallida

Genus image · Cirad · Public domain
Range not recordedhardwood1,363 lbf*44.7 lb/ft³*
Gambel oak

Quercus gambelii

Genus image · Cirad · Public domain
Range not recordedhardwood1,538 lbf*47.3 lb/ft³*
Asiahardwood2,890 lbf63.0 lb/ft³
Garapa

Apuleia leiocarpa = Apuleia molaris

Cirad · Public domain
Tropical Americahardwood1,863 lbf54.9 lb/ft³
Garcinia

Garcinia myrtifolia

Genus image · Cirad · Public domain
Range not recordedhardwood2,367 lbf*57.7 lb/ft³*
Garcinia xanthochymus

Garcinia xanthochymus

Genus image · Cirad · Public domain
Range not recordedhardwood2,530 lbf*59.6 lb/ft³*
Range not recordedhardwood1,007 lbf*38.8 lb/ft³*
Garrote

Brosimum sp

Genus image · Cirad · Public domain
Tropical Americahardwood1,074 lbf36.2 lb/ft³
Gasu

Palaquium stehlinii

Genus image · Cirad · Public domain
Range not recordedhardwood1,007 lbf*38.8 lb/ft³*
Gatae palagi

Erythrina subumbrans

Genus image · Cirad · Public domain
Range not recordedhardwood216 lbf*19.0 lb/ft³*
Gaudichauds senna

Senna gaudichaudii

Genus image · Cirad · Public domain
Range not recordedhardwood1,852 lbf*51.5 lb/ft³*
Gedu Nohor

Entandrophragma angolense

Cirad · Public domain
Africahardwood940 lbf34.0 lb/ft³
Geronggang

Cratoxylon arborescens

Asiahardwood573 lbf*30.0 lb/ft³
Geyer willow

Salix geyeriana

Genus image · G-Lignum · CC0
Range not recordedhardwood451 lbf*26.7 lb/ft³*
Gia verde

Casearia arborea

Genus image · Cirad · Public domain
Range not recordedhardwood1,475 lbf*46.4 lb/ft³*
Giant sequoia

Sequoiadendron giganteum

Marie-Lan Nguyen · Public domain
Range not recordedsoftwood408 lbf*25.1 lb/ft³*
Range not recordedhardwood832 lbf*35.5 lb/ft³*
Glícia

Glycydendron amazonicum

Cirad · Public domain
Tropical Americahardwood1,671 lbf51.5 lb/ft³*
Range not recordedhardwood1,203 lbf*42.1 lb/ft³*
Gmelina

Gmelina arborea

Cirad · Public domain
Asiahardwood622 lbf30.0 lb/ft³
Range not recordedhardwood1,363 lbf*44.7 lb/ft³*
Goatwood

Cassipourea guianensis

Cirad · Public domain
Range not recordedhardwood2,210 lbf*55.9 lb/ft³*
Gogó-de-guariba

Rauvolfia paraensis

Genus image · Cirad · Public domain
Tropical Americahardwood1,203 lbf*44.3 lb/ft³
Goiabão

Chrysophyllum lucentifolium = Pouteria pachycarpa

Cirad · Public domain
Tropical Americahardwood2,646 lbf58.1 lb/ft³
Range not recordedhardwood1,103 lbf*40.5 lb/ft³*
Golden shower

Cassia fistula

Genus image · Cirad · Public domain
Range not recordedhardwood2,139 lbf*55.1 lb/ft³*
Range not recordedhardwood1,658 lbf*48.9 lb/ft³*
Range not recordedhardwood1,923 lbf*52.4 lb/ft³*
Gommier

Dacryodes excelsa

Cirad · Public domain
Tropical Americahardwood900 lbf40.0 lb/ft³
Goncalo alves

Astronium graveolens

Cirad · Public domain
Tropical Americahardwood2,160 lbf67.7 lb/ft³*
Gongolin

Ilex sideroxyloides

Cirad · Public domain
Range not recordedhardwood1,788 lbf*50.7 lb/ft³*
Goodding's ash

Fraxinus gooddingii

Genus image · Cirad · Public domain
Range not recordedhardwood1,007 lbf*38.8 lb/ft³*
Goodding's willow

Salix gooddingii

Genus image · G-Lignum · CC0
Range not recordedhardwood451 lbf*26.7 lb/ft³*
Gourka

Garcinia dulcis

Genus image · Cirad · Public domain
Range not recordedhardwood2,210 lbf*55.9 lb/ft³*
Range not recordedhardwood1,852 lbf*51.5 lb/ft³*
Granadillo bobo

Miconia prasina

Genus image · Cirad · Public domain
Range not recordedhardwood1,363 lbf*44.7 lb/ft³*
Grand eucalyptus

Eucalyptus grandis

Cirad · Public domain
Range not recordedhardwood1,309 lbf*43.8 lb/ft³*
Grand fir

Abies grandis

Genus image · Cirad · Public domain
North Americasoftwood490 lbf25.8 lb/ft³
Grandleaf seagrape

Coccoloba pubescens

Genus image · Cirad · Public domain
Range not recordedhardwood2,963 lbf*64.1 lb/ft³*
Graves oak

Quercus gravesii

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Range not recordedhardwood479 lbf*27.5 lb/ft³*
North Americahardwood753 lbf*33.9 lb/ft³*
Gray ironbark

Eucalyptus paniculata

Paul venter · CC BY-SA 3.0
Range not recordedhardwood3,647 lbf*70.6 lb/ft³*
Gray oak

Quercus grisea

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Gray or California foothill pine

Pinus sabiniana

Genus image · Cirad · Public domain
Range not recordedsoftwood532 lbf*29.8 lb/ft³*
Gray sheoak

Casuarina glauca

Genus image · Cirad · Public domain
Range not recordedhardwood2,448 lbf*58.7 lb/ft³*
Great Basin bristlecone pine

Pinus longaeva

Genus image · Cirad · Public domain
Range not recordedsoftwood599 lbf*32.3 lb/ft³*
Great leucaene

Leucaena pulverulenta

Genus image · Cirad · Public domain
Range not recordedhardwood1,363 lbf*44.7 lb/ft³*
Range not recordedhardwood479 lbf*27.5 lb/ft³*
Green ash

Fraxinus pennsylvanica

Genus image · Cirad · Public domain
North Americahardwood1,200 lbf39.1 lb/ft³
Green wattle

Acacia decurrens

Genus image · Cirad · Public domain
Range not recordedhardwood1,054 lbf*39.6 lb/ft³*
Greene's mountain ash

Sorbus scopulina

Genus image · Cirad · Public domain
Range not recordedhardwood1,054 lbf*39.6 lb/ft³*
Greenheart

Chlorocardium rodiei

Cirad · Public domain
Tropical Americahardwood2,350 lbf64.1 lb/ft³*
Greenheart, common snakebark

Colubrina arborescens

Genus image · Cirad · Public domain
Range not recordedhardwood1,725 lbf*49.9 lb/ft³*
Grumixava

Micropholis spp.

Genus image · Cirad · Public domain
Tropical Americahardwood1,490 lbf46.0 lb/ft³