Wood Record

Brush Box vs Cabreúva-parda

Tristania spp. against Myrocarpus frondosus. Every number below names the publication it came from.

PropertyBrush BoxCabreúva-parda
Janka hardness3,088 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)3,075 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)57.4 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture26,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)22,359 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.68 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.19 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,700 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)12,460 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)—11.3%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.90Chudnoff 1984, Tropical Timbers of the World (AH-607)1.59LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Cabreúva-parda moves more evenly. Its tangential-to-radial ratio is 1.6 against 1.9, so it is the safer choice for a wide flat panel.
  • Brush Box carries 17% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.