Wood Record

Brush Box vs Casuarina

Tristania spp. against Casuarina spp.. Every number below names the publication it came from.

PropertyBrush BoxCasuarina
Janka hardness3,088 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)3,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)64.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture26,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)25,000 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.68 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)3.31 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength11,700 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)11,000 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)——
Tangential / radial ratio(lower is better)1.90Chudnoff 1984, Tropical Timbers of the World (AH-607)—

What the numbers mean

  • The two match on hardness, within 4%. Choose on movement or on appearance instead.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons