Wood Record

Brush Box vs Ingá

Tristania spp. against Inga paraensis. Every number below names the publication it came from.

PropertyBrush BoxIngá
Janka hardness3,088 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)3,064 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)65.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture26,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)26,540 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.68 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.60 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,700 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)12,090 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)—15.9%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.90Chudnoff 1984, Tropical Timbers of the World (AH-607)2.02LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons