Tristania spp. against Handroanthus serratifolius = Tabebuia serratifolia. Every number below names the publication it came from.
| Property | Brush Box | Ipê |
|---|---|---|
| Janka hardness | 3,088 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 3,100 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 72.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 26,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 24,549 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.68 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 1.86 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 11,700 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 12,360 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | — | 10.1%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.90Chudnoff 1984, Tropical Timbers of the World (AH-607) | 1.34LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 0%. Choose on movement or on appearance instead.
- Ipê moves more evenly. Its tangential-to-radial ratio is 1.3 against 1.9, so it is the safer choice for a wide flat panel.
- Ipê is the heavier of the two by 168 kg/m³, which a reader building a door or a case should weigh.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.