Wood Record

Curupay vs Jataipeba

Anadenanthera macrocarpa against Dialium guianense. Every number below names the publication it came from.

PropertyCurupayJataipeba
Janka hardness3,840 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)3,650 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC66.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)63.7 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture29,290 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)24,614 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.60 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.35 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength14,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)12,481 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)12.0%Chudnoff 1984, Tropical Timbers of the World (AH-607)14.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.65Chudnoff 1984, Tropical Timbers of the World (AH-607)1.75LPF/SFB Madeiras Brasileiras

What the numbers mean

  • Curupay resists denting better. It tests 5% harder than Jataipeba.
  • Curupay carries 19% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.