Curupay vs Miraúba
Anadenanthera macrocarpa against Mouriri collocarpa. Every number below names the publication it came from.
| Property | Curupay | Miraúba |
|---|---|---|
| Janka hardness | 3,840 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 4,032 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 66.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 68.0 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 29,290 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 27,309 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.60 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 2.49 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 14,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 13,697 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 12.0%Chudnoff 1984, Tropical Timbers of the World (AH-607) | 17.4%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.65Chudnoff 1984, Tropical Timbers of the World (AH-607) | 1.56LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Miraúba resists denting better. It tests 5% harder than Curupay.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.