The family Dipterocarpaceae supplies 13 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

13 of 13 carry a published Janka test.

WoodJankaDensity
ChengalBalanocarpus spp.2,130 lbf58.0 lb/ft³
Dark red merantiShorea spp.780 lbf53.0 lb/ft³
KapurDryobalanops spp.1,230 lbf49.9 lb/ft³
KeruingDipterocarpus spp.1,270 lbf54.2 lb/ft³
Light red merantiShorea spp.460 lbf25.1 lb/ft³
MersawaAnisoptera spp.1,290 lbf40.0 lb/ft³
ResakCotylelobium spp.1,550 lbf52.0 lb/ft³
ShoreaShorea spp., bullau group1,780 lbf53.3 lb/ft³
ThinganHopea spp.1,255 lbf48.0 lb/ft³
White lauanPentacme contorta690 lbf33.0 lb/ft³
White merantiShorea spp.1,140 lbf42.1 lb/ft³
White SerayaParashorea spp.838 lbf33.0 lb/ft³
Yellow merantiShorea spp.770 lbf34.7 lb/ft³