Wood Record

family

Fabaceae

The family Fabaceae supplies 135 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

25 of 135 carry a published Janka test.

WoodJankaDensity
Amur maackiaMaackia amurensis1,475 lbf*46.4 lb/ft³
Anadenanthera peregrinaAnadenanthera peregrina2,064 lbf*54.2 lb/ft³
Andira-uxiAndira surinamensis = Andira retusa1,788 lbf43.7 lb/ft³
AngelimHymenolobium sp1,422 lbf44.9 lb/ft³
Angelim-amargosoVatairea sericea2,167 lbf56.2 lb/ft³
Angelim-pedraHymenolobium modestum1,647 lbf50.7 lb/ft³
Angelim-pedraHymenolobium petraeum1,301 lbf44.3 lb/ft³
Angelim-pedraHymenolobium pulcherrimum1,206 lbf44.3 lb/ft³
Angelim-pedraHymenolobium nitidum1,257 lbf43.1 lb/ft³
Angelim-tintoAndira sp1,989 lbf56.2 lb/ft³
Apple blossomCassia javanica1,725 lbf*49.9 lb/ft³
Argentine sennaSenna corymbosa1,309 lbf*43.8 lb/ft³
AuriAcacia auriculiformis1,598 lbf*48.1 lb/ft³
Black locustRobinia pseudoacacia1,700 lbf48.3 lb/ft³
Black wattleAcacia mangium1,007 lbf*38.8 lb/ft³
Black wattleAcacia mearnsii1,990 lbf*53.3 lb/ft³
Blackbead ebonyEbenopsis ebano3,749 lbf*71.5 lb/ft³
BloodwoodtreeHaematoxylum campechianum3,054 lbf*65.0 lb/ft³
Brazilian tulipwoodDalbergia decipularis2,963 lbf*64.1 lb/ft³
Bristly locustRobinia hispida1,852 lbf*51.5 lb/ft³
Broadleaf lancepodLonchocarpus heptaphyllus1,923 lbf*52.4 lb/ft³
BucayoErythrina fusca255 lbf*20.5 lb/ft³
Butterfly treeBauhinia purpurea1,103 lbf*40.5 lb/ft³
Cabreúva-pardaMyrocarpus frondosus3,075 lbf57.4 lb/ft³
California redbudCercis orbiculata1,054 lbf*39.6 lb/ft³
Casia amarillaSenna spectabilis1,007 lbf*38.8 lb/ft³
Catclaw blackbeadPithecellobium unguis-cati2,210 lbf*55.9 lb/ft³
CercipoMyrospermum frutescens3,336 lbf*67.7 lb/ft³
CerejeiraAmburana acreana880 lbf35.6 lb/ft³
ChedebsungelOrmosia calavensis1,054 lbf*39.6 lb/ft³
Chinese albiziaAlbizia chinensis608 lbf*30.7 lb/ft³
CocoboloDalbergia tucurensis1,990 lbf*53.3 lb/ft³
Cojoba arboreaCojoba arborea1,475 lbf*46.4 lb/ft³
CopaibaCopaifera officinalis1,475 lbf*46.4 lb/ft³
Coral erythrinaErythrina corallodendron216 lbf*19.0 lb/ft³
CrybabytreeErythrina crista-galli255 lbf*20.5 lb/ft³
CumaruDipteryx odorata3,415 lbf66.8 lb/ft³
Desert ironwoodOlneya tesota4,196 lbf*75.4 lb/ft³
Dragonsblood treePterocarpus officinalis875 lbf*36.3 lb/ft³
Eastern redbudCercis canadensis1,103 lbf*40.5 lb/ft³
Egyptian riverhempSesbania sesban573 lbf*29.8 lb/ft³
Elegant mimosaMimosa arenosa2,779 lbf*62.2 lb/ft³
Embira-de-preguiçaPterocarpus sp.1,731 lbf33.0 lb/ft³
False sicklepodSenna multijuga791 lbf*34.7 lb/ft³
False tamarindLysiloma latisiliquum1,255 lbf*43.0 lb/ft³
Faveira-amargosaVatairea paraensis2,174 lbf62.2 lb/ft³
Faveira-amargosaVatairea guianensis1,532 lbf51.8 lb/ft³
Faveira-amargosaVataireopsis speciosa1,043 lbf46.2 lb/ft³
Fishpoison treePiscidia piscipula1,990 lbf*53.3 lb/ft³
Flor de San JoseSenna atomaria1,658 lbf*48.9 lb/ft³
FusticPictetia aculeata2,139 lbf*55.1 lb/ft³
GarapaApuleia leiocarpa = Apuleia molaris1,863 lbf54.9 lb/ft³
Gatae palagiErythrina subumbrans216 lbf*19.0 lb/ft³
Gaudichauds sennaSenna gaudichaudii1,852 lbf*51.5 lb/ft³
Golden showerCassia fistula2,139 lbf*55.1 lb/ft³
Great leucaeneLeucaena pulverulenta1,363 lbf*44.7 lb/ft³
Green wattleAcacia decurrens1,054 lbf*39.6 lb/ft³
GulosCynometra ramiflora2,287 lbf*56.9 lb/ft³
HaujilloHavardia pallens2,287 lbf*56.9 lb/ft³
Honey mesquiteProsopis glandulosa2,779 lbf*62.2 lb/ft³
HoneylocustGleditsia triacanthos1,580 lbf46.4 lb/ft³
Ice cream beanInga edulis1,054 lbf*39.6 lb/ft³
IfiInocarpus fagifer960 lbf*38.0 lb/ft³
IfileleIntsia bijuga1,788 lbf*50.7 lb/ft³
Indian rosewoodDalbergia sissoo1,598 lbf*48.1 lb/ft³
Inga nobilisInga nobilis1,363 lbf*44.7 lb/ft³
JandProsopis cineraria1,538 lbf*47.3 lb/ft³
Japanese pagoda treeStyphnolobium japonicum1,419 lbf*45.5 lb/ft³
Jerusalem thornParkinsonia aculeata1,255 lbf*43.0 lb/ft³
Kentucky coffeetreeGymnocladus dioicus1,103 lbf*40.5 lb/ft³
KingwoodDalbergia cearensis2,607 lbf*60.4 lb/ft³
KisaksPongamia pinnata1,309 lbf*43.8 lb/ft³
KoaAcacia koa2,287 lbf*56.9 lb/ft³
Littleleaf leadtreeLeucaena retusa1,054 lbf*39.6 lb/ft³
Malabar kinoPterocarpus marsupium2,210 lbf*55.9 lb/ft³
MamaniSophora chrysophylla2,867 lbf*63.1 lb/ft³
MelancieiraAlexa grandiflora1,424 lbf46.4 lb/ft³
Mescal beanSophora secundiflora1,475 lbf*46.4 lb/ft³
MimosaAlbizia julibrissin875 lbf*36.3 lb/ft³
MonkeypodPithecellobium dulce1,538 lbf*47.3 lb/ft³
Mountain ebonyBauhinia variegata1,255 lbf*43.0 lb/ft³
Mountain immortelleErythrina poeppigiana321 lbf*22.8 lb/ft³
MulgaAcacia aneura3,749 lbf*71.5 lb/ft³
Naked albiziaAlbizia carbonaria1,007 lbf*38.8 lb/ft³
Napoleon's plumeBauhinia monandra1,309 lbf*43.8 lb/ft³
New Mexico locustRobinia neomexicana1,852 lbf*51.5 lb/ft³
Palo de hozMachaerium lunatum149 lbf*15.9 lb/ft³
Parkia timorianaParkia timoriana608 lbf*30.7 lb/ft³
Pau-santoZollernia paraensis3,261 lbf78.7 lb/ft³
Peltophorum pterocarpumPeltophorum pterocarpum1,363 lbf*44.7 lb/ft³
Pericopsis moonianaPericopsis mooniana2,530 lbf*59.6 lb/ft³
PeroniaOrmosia krugii753 lbf*33.9 lb/ft³
Petite flamboyant bauhiniaBauhinia multinervia2,139 lbf*55.1 lb/ft³
Philippine pigeonwingsClitoria fairchildiana1,363 lbf*44.7 lb/ft³
Pink showerCassia grandis1,852 lbf*51.5 lb/ft³
Prickly MosesAcacia verticillata1,054 lbf*39.6 lb/ft³
Pride-of-BarbadosCaesalpinia pulcherrima1,598 lbf*48.1 lb/ft³
QuickstickGliricidia sepium2,287 lbf*56.9 lb/ft³
RaintreeSamanea saman1,103 lbf*40.5 lb/ft³
Red beadtreeAdenanthera pavonina1,598 lbf*48.1 lb/ft³
River kokoInga vera1,007 lbf*38.8 lb/ft³
Royal poincianaDelonix regia641 lbf*31.5 lb/ft³
Sacky sac beanInga laurina1,788 lbf*50.7 lb/ft³
Screwbean mesquiteProsopis pubescens2,779 lbf*62.2 lb/ft³
SennaSenna septemtrionalis1,309 lbf*43.8 lb/ft³
Siamese cassiaSenna siamea1,990 lbf*53.3 lb/ft³
Siamese rosewoodDalbergia cochinchinensis3,441 lbf*68.7 lb/ft³
Silver bushSophora tomentosa1,363 lbf*44.7 lb/ft³
Silver wattleAcacia dealbata1,054 lbf*39.6 lb/ft³
Small Philippine acaciaAcacia confusa2,367 lbf*57.7 lb/ft³
St. John's breadCeratonia siliqua1,363 lbf*44.7 lb/ft³
St. Thomas treeBauhinia tomentosa2,692 lbf*61.3 lb/ft³
StinkwoodPiscidia carthagenensis1,852 lbf*51.5 lb/ft³
SucupiraBowdichia nitida2,903 lbf59.9 lb/ft³
SucupiraDiplotropis purpurea2,140 lbf56.2 lb/ft³
Sydney golden wattleAcacia longifolia1,538 lbf*47.3 lb/ft³
Tall albiziaAlbizia procera1,538 lbf*47.3 lb/ft³
TamarindTamarindus indica2,692 lbf*61.3 lb/ft³
TentoOrmosia paraensis1,688 lbf45.6 lb/ft³
TentoOrmosia coccinea1,378 lbf44.9 lb/ft³
Texas paloverdeParkinsonia texana1,725 lbf*49.9 lb/ft³
TexasplumeBauhinia lunarioides2,058 lbf*54.1 lb/ft³
Tiger's clawErythrina variegata197 lbf*18.2 lb/ft³
TipaTipuana tipu1,363 lbf*44.7 lb/ft³
Ukall ra ngebardAlbizia retusa1,103 lbf*40.5 lb/ft³
UrucuranaSwartzia recurva2,469 lbf57.4 lb/ft³
ValamuertoSenna pendula1,852 lbf*51.5 lb/ft³
Vegetable hummingbirdSesbania grandiflora608 lbf*30.7 lb/ft³
Velvet mesquiteProsopis velutina2,779 lbf*62.2 lb/ft³
WaterlocustGleditsia aquatica1,475 lbf*46.4 lb/ft³
White leadtreeLeucaena leucocephala1,658 lbf*48.9 lb/ft³
Whiteflower albiziaAlbizia saponaria1,309 lbf*43.8 lb/ft³
Wili wiliErythrina sandwicensis276 lbf*21.2 lb/ft³
Woman's tongueAlbizia lebbeck1,363 lbf*44.7 lb/ft³
YellowwoodCladrastis kentukea1,538 lbf*47.3 lb/ft³