Wood Record

family

Leguminosae

The family Leguminosae supplies 80 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

58 of 80 carry a published Janka test.

WoodJankaDensity
AdoungMonopetalanthus heitzii542 lbf*33.0 lb/ft³
African BlackwoodDalbergia melanoxylon—83.0 lb/ft³
African PadaukPterocarpus soyauxii1,538 lbf*46.0 lb/ft³
AfrormosiaPericopsis elata1,560 lbf43.0 lb/ft³
AfzeliaAfzelia spp.1,810 lbf51.0 lb/ft³
AgbaGossweilerodendron balsamiferum740 lbf30.0 lb/ft³
AlbizziaAlbizia spp.955 lbf40.0 lb/ft³
AmburanaAmburana cearensis790 lbf42.1 lb/ft³
AmendoimPterogyne nitens1,852 lbf*50.0 lb/ft³
Andaman PadaukPterocarpus dalbergioides1,630 lbf48.9 lb/ft³
AngelinAndira inermis1,750 lbf52.0 lb/ft³
AngeliqueDicorynia guianensis1,290 lbf50.0 lb/ft³
AraribaCentrolobium spp.1,030 lbf50.0 lb/ft³
AromataClathrotropis spp-2,960 lbf72.0 lb/ft³
Australian BlackwoodAcacia melanoxylon1,100 lbf40.0 lb/ft³
AyanDistemonanthus benthamianus1,230 lbf45.0 lb/ft³
BalsamoMyroxylon balsamum2,200 lbf58.0 lb/ft³
BanuyoWallaceodendron celebicum1,309 lbf*44.0 lb/ft³
BaracaraOrmosia spp.1,000 lbf44.0 lb/ft³
BataiAlbizia falcataria344 lbf*24.0 lb/ft³
BengeGuibourtia arnoldiana1,750 lbf50.0 lb/ft³
BerliniaBerlinia spp.1,360 lbf44.7 lb/ft³
Bitter AngelimVatairea spp.1,250 lbf46.0 lb/ft³
Black Cabbage-BarkLonchocarpus spp.2,700 lbf52.0 lb/ft³
Black WattleAcacia mollissima1,750 lbf45.0 lb/ft³
Brazilian rosewoodDalbergia nigra2,720 lbf64.1 lb/ft³
BubingaGuibourtia spp.2,690 lbf55.9 lb/ft³
BurkeaBurkea africana2,139 lbf*54.0 lb/ft³
Burma PadaukPterocarpus macrocarpus2,170 lbf54.0 lb/ft³
CarboneroPiptadenia pittieri1,615 lbf46.0 lb/ft³
CativoPrioria copaifera630 lbf30.0 lb/ft³
CaviunaMachaerium spp.2,139 lbf*53.0 lb/ft³
Cedro-RanaCedrelinga catenaeformis1,103 lbf*40.5 lb/ft³
CocoboloDalbergia retusa3,860 lbf*69.0 lb/ft³
CordylaCordyla africana1,580 lbf54.0 lb/ft³
CurupayAnadenanthera macrocarpa3,840 lbf66.0 lb/ft³
DahomaPiptadeniastrum africanum1,540 lbf43.0 lb/ft³
DinaSwartzia fistuloides3,147 lbf*64.0 lb/ft³
DjedoeSclerolobium spp.700 lbf35.0 lb/ft³
EkopTetraberlinia tubmaniana1,475 lbf*46.0 lb/ft³
EyoumDialium dinklagei2,287 lbf*56.0 lb/ft³
GuachapelePseudosamanea guachapele1,255 lbf*41.0 lb/ft³
GuanacasteEnterolobium cyclocarpum520 lbf26.0 lb/ft³
HaiariAlexa imperatricis690 lbf38.4 lb/ft³
Honduras RosewoodDalbergia stevensonii3,097 lbf*63.0 lb/ft³
Indian rosewoodDalbergia latifolia3,170 lbf53.0 lb/ft³
KempasKoompassia malaccensis1,710 lbf55.0 lb/ft³
KeranjiDialium spp.2,963 lbf*60.0 lb/ft³
KokkoAlbizia lebbek1,240 lbf39.0 lb/ft³
MacawoodPlatymiscium spp.3,150 lbf64.0 lb/ft³
MbarikaIsoberlinia schaffleri1,420 lbf50.0 lb/ft³
MerbauIntsia spp.1,500 lbf50.0 lb/ft³
MissandaErythrophleum ivorense2,930 lbf56.0 lb/ft³
MoraMora spp.2,300 lbf62.0 lb/ft³
MtunduBrachystegia spiciformis1,830 lbf51.0 lb/ft³
MuhimbiCynometra alexandri2,975 lbf54.0 lb/ft³
MuningaPterocarpus angolensis1,480 lbf41.0 lb/ft³
MuwaJulbernardia globiflora2,470 lbf60.0 lb/ft³
NarraPterocarpus indicus1,202 lbf40.0 lb/ft³
NkobakobaBaikiaea insignis subsp. minor1,770 lbf50.0 lb/ft³
OgeaDan i el lia ogea710 lbf31.0 lb/ft³
OkanCylicodiscus gabunensis2,780 lbf64.1 lb/ft³
OkwenBrachystegia spp.1,180 lbf39.0 lb/ft³
OvangkolGuibourtia ehie1,923 lbf*52.0 lb/ft³
Panga PangaMillettia spp.1,630 lbf55.0 lb/ft³
Para-angelimHymenolobium excelsum1,720 lbf47.0 lb/ft³
PartridgewoodCaesalplnia spp.5,868 lbf*78.0 lb/ft³
PurpleheartPeltogyne spp.1,860 lbf58.0 lb/ft³
PyinkadoXylia xylocarpa2,248 lbf61.0 lb/ft³
Rhodesian-TeakBaikiaea plurijuga2,990 lbf56.0 lb/ft³
SabicúLyslloma spp.1,400 lbf48.0 lb/ft³
SamánPithecellobium saman850 lbf35.0 lb/ft³
SapoDidelotia brevipaniculata1,103 lbf*41.0 lb/ft³
SepetirPseudosindora palustris1,410 lbf42.0 lb/ft³
SucupiraBowdichia spp.2,448 lbf*58.7 lb/ft³
TchitolaOxystigma oxyphyllum1,250 lbf40.0 lb/ft³
WacapouVouacapoua americana2,867 lbf*59.0 lb/ft³
WallabaEperua spp.2,040 lbf58.0 lb/ft³
WamaraSwartzia spp.3,692 lbf70.0 lb/ft³
ZebranoMicroberlinia brazzavillensis2,139 lbf*53.0 lb/ft³