family
Moraceae
The family Moraceae supplies 62 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
24 of 62 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| African CorkwoodMusanga cecropioides | 165 lbf* | 18.0 lb/ft³ |
| Amapá-doceBrosimum parinarioides | 1,250 lbf | 43.8 lb/ft³ |
| Amapá-doceBrosimum potabile | 1,184 lbf | 40.5 lb/ft³ |
| AmateFicus obtusifolia | 608 lbf* | 30.7 lb/ft³ |
| Amora / amoreiraMaclura tinctoria | 2,385 lbf | 56.8 lb/ft³ |
| AntíarisAntiaris spp- | 500 lbf | 27.0 lb/ft³ |
| AoaFicus obliqua | 791 lbf* | 34.7 lb/ft³ |
| AoaFicus prolixa | 423 lbf* | 26.0 lb/ft³ |
| Artocarpus heterophyllusArtocarpus heterophyllus | 875 lbf* | 36.3 lb/ft³ |
| Black mulberryMorus nigra | 1,152 lbf* | 41.3 lb/ft³ |
| BreadfruitArtocarpus altilis | 451 lbf* | 26.7 lb/ft³ |
| Brown-woolly figFicus drupacea | 369 lbf* | 24.3 lb/ft³ |
| CapomoBrosimum spp. (Alicastrum group) | 1,340 lbf | 49.4 lb/ft³ |
| CauchoCastilla ulei | 313 lbf | 29.3 lb/ft³ |
| Chinese banyanFicus microcarpa | 1,103 lbf* | 40.5 lb/ft³ |
| Chinese banyanFicus thonningii | 791 lbf* | 34.7 lb/ft³ |
| Conduru / pau-vermelhoBrosimum rubescens | 2,062 lbf | 50.6 lb/ft³ |
| DifouMorus mesozygia | 2,139 lbf* | 54.0 lb/ft³ |
| Edible figFicus carica | 714 lbf* | 33.1 lb/ft³ |
| False breadnutPseudolmedia spuria | 2,530 lbf* | 59.6 lb/ft³ |
| Ficus copiosaFicus copiosa | 915 lbf* | 37.1 lb/ft³ |
| Ficus luteaFicus lutea | 479 lbf* | 27.5 lb/ft³ |
| Figueira / gameleiraFicus insipida | 269 lbf | 28.1 lb/ft³ |
| Florida strangler figFicus aurea | 753 lbf* | 33.9 lb/ft³ |
| FusticChlorophora tinctoria | 2,380 lbf | 56.0 lb/ft³ |
| GarroteBrosimum sp | 1,074 lbf | 36.2 lb/ft³ |
| GuariúbaClarisia racemosa | 1,380 lbf | 41.2 lb/ft³ |
| Hawaii roughbushStreblus pendulinus | 1,788 lbf* | 50.7 lb/ft³ |
| HigoFicus virens | 608 lbf* | 30.7 lb/ft³ |
| Indian banyanFicus benghalensis | 791 lbf* | 34.7 lb/ft³ |
| Indian rubberplantFicus elastica | 960 lbf* | 38.0 lb/ft³ |
| IrokoChlorophora spp. | 1,260 lbf | 43.0 lb/ft³ |
| Jaguey blancoFicus trigonata | 714 lbf* | 33.1 lb/ft³ |
| Jamaican cherry figFicus americana | 608 lbf* | 30.7 lb/ft³ |
| JanitáBrosimum alicastrum | 2,059 lbf | 58.7 lb/ft³ |
| Janitá / garroteBrosimum utile | 946 lbf | 36.2 lb/ft³ |
| KeledangArtocarpus spp. | 1,250 lbf | 44.0 lb/ft³ |
| Leche PerraHelicostylis tomentosa | 2,700 lbf | 55.0 lb/ft³ |
| LetterwoodPiratlnera guianensis | 4,669 lbf* | 74.0 lb/ft³ |
| MarangArtocarpus odoratissimus | 1,152 lbf* | 41.3 lb/ft³ |
| MastatePoulsenia armata | 360 lbf | 25.0 lb/ft³ |
| MatiFicus tinctoria | 791 lbf* | 34.7 lb/ft³ |
| MuiratingaMaquira sclerophylla | 1,389 lbf | 43.8 lb/ft³ |
| MururéBrosimum gaudichaudii | 3,036 lbf | 56.8 lb/ft³ |
| MururéBrosimum acutifolium subsp interjectum | 1,120 lbf | 42.1 lb/ft³ |
| Osage orangeMaclura pomifera | 2,607 lbf* | 60.4 lb/ft³ |
| Panama rubbertreeCastilla elastica | 423 lbf* | 26.0 lb/ft³ |
| Paper mulberryBroussonetia papyrifera | 542 lbf* | 29.1 lb/ft³ |
| Peepul treeFicus religiosa | 679 lbf* | 32.3 lb/ft³ |
| Port Jackson figFicus rubiginosa | 679 lbf* | 32.3 lb/ft³ |
| RamónTrophis spp. | 770 lbf | 40.0 lb/ft³ |
| Red mulberryMorus rubra | 1,152 lbf* | 41.3 lb/ft³ |
| Roxburgh figFicus auriculata | 714 lbf* | 33.1 lb/ft³ |
| SandeBrosimum spp., utile group | 900 lbf | 37.1 lb/ft³ |
| Sycamore figFicus sycomorus | 791 lbf* | 34.7 lb/ft³ |
| TatajubaBagassa guianensis | 1,660 lbf | 55.1 lb/ft³ |
| Texas mulberryMorus microphylla | 1,598 lbf* | 48.1 lb/ft³ |
| Trumpet-WoodCecropia peltata | 320 lbf | 23.0 lb/ft³ |
| Weeping figFicus benjamina | 915 lbf* | 37.1 lb/ft³ |
| White mulberryMorus alba | 1,363 lbf* | 44.7 lb/ft³ |
| White ramoonTrophis racemosa | 1,658 lbf* | 48.9 lb/ft³ |
| Wild banyantree, shortleaf figFicus citrifolia | 832 lbf* | 35.5 lb/ft³ |