The family Myrtaceae supplies 74 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

8 of 74 carry a published Janka test.

WoodJankaDensity
AllspicePimenta dioica3,441 lbf*68.7 lb/ft³
AppleboxEucalyptus bridgesiana2,367 lbf*57.7 lb/ft³
Argyle appleEucalyptus cinerea2,210 lbf*55.9 lb/ft³
AsiSyzygium inophylloides2,367 lbf*57.7 lb/ft³
Australian tallowwoodEucalyptus microcorys3,054 lbf*65.0 lb/ft³
BayrumtreePimenta racemosa3,147 lbf*65.9 lb/ft³
BirdcherryEugenia monticola2,779 lbf*62.2 lb/ft³
Black ironboxEucalyptus raveretiana3,539 lbf*69.7 lb/ft³
BlackbuttEucalyptus pilularis1,923 lbf*52.4 lb/ft³
BlackrodwoodEugenia biflora1,990 lbf*53.3 lb/ft³
BluegumEucalyptus globulus2,060 lbf64.1 lb/ft³
Broad-Leaved Tea-TreeMelaleuca quinquenervia1,788 lbf*50.0 lb/ft³
Broom teatreeLeptospermum scoparium2,287 lbf*56.9 lb/ft³
Brush BoxTristania spp.3,088 lbf62.0 lb/ft³
Brush cherrySyzygium paniculatum1,598 lbf*48.1 lb/ft³
BurganKunzea ericoides2,064 lbf*54.2 lb/ft³
Cajeput treeMelaleuca linariifolia1,054 lbf*39.6 lb/ft³
Christmas cherryEugenia pseudopsidium2,448 lbf*58.7 lb/ft³
CieneguilloMyrcia deflexa2,692 lbf*61.3 lb/ft³
Corymbia citriodoraCorymbia citriodora2,867 lbf*63.1 lb/ft³
DegluptaEucalyptus deglupta470 lbf42.0 lb/ft³
FeijoaFeijoa sellowiana1,788 lbf*50.7 lb/ft³
Forest redgumEucalyptus tereticornis2,367 lbf*57.7 lb/ft³
Grand eucalyptusEucalyptus grandis1,309 lbf*43.8 lb/ft³
Gray ironbarkEucalyptus paniculata3,647 lbf*70.6 lb/ft³
GuavaPsidium guajava1,475 lbf*46.4 lb/ft³
GuavaberryMyrciaria floribunda2,692 lbf*61.3 lb/ft³
Hoja menudaSiphoneugena densiflora2,779 lbf*62.2 lb/ft³
JarrahEucalyptus marginata1,910 lbf54.0 lb/ft³
Java plumSyzygium cumini1,658 lbf*48.9 lb/ft³
KarriEucalyptus diversicolor2,040 lbf57.0 lb/ft³
KelatEugenia spp.1,198 lbf50.0 lb/ft³
LathberryEugenia cordata2,692 lbf*61.3 lb/ft³
Malaysian appleSyzygium malaccense1,007 lbf*38.8 lb/ft³
Manna gumEucalyptus viminalis1,923 lbf*52.4 lb/ft³
Mountain graygumEucalyptus goniocalyx2,287 lbf*56.9 lb/ft³
Narrowleaf red ironbarkEucalyptus crebra2,692 lbf*61.3 lb/ft³
OhiaMetrosideros collina subsp. polymorpha2,090 lbf57.0 lb/ft³
Ohia haSyzygium sandwicense1,990 lbf*53.3 lb/ft³
Ohia lehuaMetrosideros polymorpha1,923 lbf*52.4 lb/ft³
Pale lidflowerCalyptranthes pallens2,607 lbf*60.4 lb/ft³
Privet stopperEugenia ligustrina2,692 lbf*61.3 lb/ft³
PunchberryMyrcia splendens2,210 lbf*55.9 lb/ft³
Red bloodwoodCorymbia gummifera2,139 lbf*55.1 lb/ft³
Red ironbarkEucalyptus sideroxylon3,147 lbf*65.9 lb/ft³
Red rodwoodMyrcia citrifolia2,692 lbf*61.3 lb/ft³
Redberry stopperEugenia confusa3,241 lbf*66.9 lb/ft³
RedboxEucalyptus polyanthemos2,867 lbf*63.1 lb/ft³
RedgumCorymbia calophylla1,658 lbf*48.9 lb/ft³
RedmahoganyEucalyptus resinifera2,287 lbf*56.9 lb/ft³
River red gumEucalyptus camaldulensis1,990 lbf*53.3 lb/ft³
RockmyrtleEugenia procera2,692 lbf*61.3 lb/ft³
Rose myrtleRhodomyrtus tomentosa1,923 lbf*52.4 lb/ft³
Roundleaf gumEucalyptus deanei1,852 lbf*51.5 lb/ft³
Sea appleSyzygium grande1,054 lbf*39.6 lb/ft³
Serrette guaveEugenia domingensis1,788 lbf*50.7 lb/ft³
Silver-dollar eucalyptusEucalyptus cordata1,054 lbf*39.6 lb/ft³
Southern mahoganyEucalyptus botryoides2,064 lbf*54.2 lb/ft³
Spotted gumCorymbia maculata2,448 lbf*58.7 lb/ft³
Stahl's stopperEugenia stahlii2,287 lbf*56.9 lb/ft³
Strawberry guavaPsidium cattleianum2,779 lbf*62.2 lb/ft³
SugargumEucalyptus cladocalyx2,867 lbf*63.1 lb/ft³
Surinam cherryEugenia uniflora3,147 lbf*65.9 lb/ft³
SwampmahoganyEucalyptus robusta1,788 lbf*50.7 lb/ft³
Sydney bluegumEucalyptus saligna1,419 lbf*45.5 lb/ft³
Syzygium jambosSyzygium jambos1,598 lbf*48.1 lb/ft³
TuartEucalyptus gomphocephala2,530 lbf*59.6 lb/ft³
TurpentineSyncarpia glomulifera2,750 lbf60.0 lb/ft³
TwinberryMyrcianthes fragrans2,607 lbf*60.4 lb/ft³
VinegartreeLophostemon confertus2,139 lbf*55.1 lb/ft³
Western Australian floodedgumEucalyptus rudis1,475 lbf*46.4 lb/ft³
White ironbarkEucalyptus leucoxylon2,692 lbf*61.3 lb/ft³
White stopperEugenia axillaris2,064 lbf*54.2 lb/ft³
YateEucalyptus cornuta3,147 lbf*65.9 lb/ft³