Wood Record

family

Sapindaceae

The family Sapindaceae supplies 57 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

6 of 57 carry a published Janka test.

WoodJankaDensity
AkeeBlighia sapida2,139 lbf*55.1 lb/ft³
Amur mapleAcer ginnala832 lbf*35.5 lb/ft³
Bigleaf mapleAcer macrophyllum850 lbf33.6 lb/ft³
Bigtooth mapleAcer grandidentatum832 lbf*35.5 lb/ft³
Black mapleAcer nigrum1,180 lbf39.8 lb/ft³
Bottlebrush buckeyeAesculus parviflora369 lbf*24.3 lb/ft³
BoxelderAcer negundo641 lbf*31.5 lb/ft³
Butterbough, inkwoodExothea paniculata2,367 lbf*57.7 lb/ft³
California buckeyeAesculus californica369 lbf*24.3 lb/ft³
CarrotwoodCupaniopsis anacardioides2,367 lbf*57.7 lb/ft³
CeboruquilloThouinia striata2,963 lbf*64.1 lb/ft³
Chalk mapleAcer leucoderme832 lbf*35.5 lb/ft³
Dimocarpus longanDimocarpus longan2,867 lbf*63.1 lb/ft³
Ebeludes, chebeludesAllophylus timorensis1,363 lbf*44.7 lb/ft³
Fa`ailiHarpullia arborea1,475 lbf*46.4 lb/ft³
FerntreeFilicium decipiens1,990 lbf*53.3 lb/ft³
Florida hopbushDodonaea viscosa3,336 lbf*67.7 lb/ft³
Florida mapleAcer barbatum832 lbf*35.5 lb/ft³
Goldenrain treeKoelreuteria bipinnata1,658 lbf*48.9 lb/ft³
Goldenrain treeKoelreuteria paniculata1,923 lbf*52.4 lb/ft³
Hedge mapleAcer campestre832 lbf*35.5 lb/ft³
Horse chestnutAesculus hippocastanum369 lbf*24.3 lb/ft³
InkwoodHypelate trifoliata2,963 lbf*64.1 lb/ft³
Japanese mapleAcer palmatum875 lbf*36.3 lb/ft³
KasaiPometia spp.1,595 lbf41.0 lb/ft³
Lac treeSchleichera oleosa2,963 lbf*64.1 lb/ft³
LycheeLitchi chinensis3,241 lbf*66.9 lb/ft³
Matayba apetalaMatayba apetala1,538 lbf*47.3 lb/ft³
Mexican buckeyeUngnadia speciosa1,363 lbf*44.7 lb/ft³
Miyabe mapleAcer miyabei832 lbf*35.5 lb/ft³
Mountain mapleAcer spicatum832 lbf*35.5 lb/ft³
Negra loraMatayba domingensis2,139 lbf*55.1 lb/ft³
Norway mapleAcer platanoides832 lbf*35.5 lb/ft³
Ohio buckeyeAesculus glabra369 lbf*24.3 lb/ft³
Painted buckeyeAesculus sylvatica369 lbf*24.3 lb/ft³
Painted mapleAcer mono832 lbf*35.5 lb/ft³
Palo de cajaAllophylus racemosus1,203 lbf*42.1 lb/ft³
Paperbark mapleAcer griseum832 lbf*35.5 lb/ft³
PulasanNephelium ramboutan-ake2,692 lbf*61.3 lb/ft³
Purple blow mapleAcer truncatum832 lbf*35.5 lb/ft³
RambutanNephelium lappaceum2,367 lbf*57.7 lb/ft³
Red buckeyeAesculus pavia369 lbf*24.3 lb/ft³
Red mapleAcer rubrum950 lbf37.8 lb/ft³
Rocky Mountain mapleAcer glabrum832 lbf*35.5 lb/ft³
Silver mapleAcer saccharinum700 lbf32.8 lb/ft³
Spanish limeMelicoccus bijugatus2,607 lbf*60.4 lb/ft³
Striped mapleAcer pensylvanicum714 lbf*33.1 lb/ft³
Sugar mapleAcer saccharum1,450 lbf44.1 lb/ft³
Sycamore mapleAcer pseudoplatanus832 lbf*35.5 lb/ft³
Tatarian mapleAcer tataricum832 lbf*35.5 lb/ft³
TavaPometia pinnata1,725 lbf*49.9 lb/ft³
Three Flower MapleAcer triflorum832 lbf*35.5 lb/ft³
Trident mapleAcer buergerianum832 lbf*35.5 lb/ft³
Vine mapleAcer circinatum832 lbf*35.5 lb/ft³
Wild ackeeCupania americana1,363 lbf*44.7 lb/ft³
Wingleaf soapberrySapindus saponaria1,788 lbf*50.7 lb/ft³
Yellow buckeyeAesculus flava369 lbf*24.3 lb/ft³