WoodJankaDensity
Amur mapleAcer ginnala832 lbf*35.5 lb/ft³
Bigleaf mapleAcer macrophyllum850 lbf33.6 lb/ft³
Bigtooth mapleAcer grandidentatum832 lbf*35.5 lb/ft³
Black mapleAcer nigrum1,180 lbf39.8 lb/ft³
BoxelderAcer negundo641 lbf*31.5 lb/ft³
Chalk mapleAcer leucoderme832 lbf*35.5 lb/ft³
Florida mapleAcer barbatum832 lbf*35.5 lb/ft³
Hedge mapleAcer campestre832 lbf*35.5 lb/ft³
Japanese mapleAcer palmatum875 lbf*36.3 lb/ft³
Miyabe mapleAcer miyabei832 lbf*35.5 lb/ft³
Mountain mapleAcer spicatum832 lbf*35.5 lb/ft³
Norway mapleAcer platanoides832 lbf*35.5 lb/ft³
Painted mapleAcer mono832 lbf*35.5 lb/ft³
Paperbark mapleAcer griseum832 lbf*35.5 lb/ft³
Purple blow mapleAcer truncatum832 lbf*35.5 lb/ft³
Red mapleAcer rubrum950 lbf37.8 lb/ft³
Rocky Mountain mapleAcer glabrum832 lbf*35.5 lb/ft³
Silver mapleAcer saccharinum700 lbf32.8 lb/ft³
Striped mapleAcer pensylvanicum714 lbf*33.1 lb/ft³
Sugar mapleAcer saccharum1,450 lbf44.1 lb/ft³
Sycamore mapleAcer pseudoplatanus832 lbf*35.5 lb/ft³
Tatarian mapleAcer tataricum832 lbf*35.5 lb/ft³
Three Flower MapleAcer triflorum832 lbf*35.5 lb/ft³
Trident mapleAcer buergerianum832 lbf*35.5 lb/ft³
Vine mapleAcer circinatum832 lbf*35.5 lb/ft³