1 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Anadenanthera peregrinaAnadenanthera peregrina | 2,064 lbf* | 54.2 lb/ft³ |
| CurupayAnadenanthera macrocarpa | 3,840 lbf | 66.0 lb/ft³ |