Woods sold under several trade names often come from one genus. These 2 share the genus Chlorophora, so they are close relatives and frequent substitutes for each other.

2 of 2 carry a published Janka test.

WoodJankaDensity
FusticChlorophora tinctoria2,380 lbf56.0 lb/ft³
IrokoChlorophora spp.1,260 lbf43.0 lb/ft³