genus
Picea
Woods sold under several trade names often come from one genus. These 10 share the genus Picea, so they are close relatives and frequent substitutes for each other.
5 of 10 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Black sprucePicea mariana | 530 lbf | 29.3 lb/ft³ |
| Blue sprucePicea pungens | 449 lbf* | 26.7 lb/ft³ |
| Brewer sprucePicea breweriana | 449 lbf* | 26.7 lb/ft³ |
| Engelmann sprucePicea engelmannii | 390 lbf | 24.5 lb/ft³ |
| Norway sprucePicea abies | 449 lbf* | 26.7 lb/ft³ |
| Red sprucePicea rubens | 530 lbf | 28.0 lb/ft³ |
| Sakhalin sprucePicea glehnii | 449 lbf* | 26.7 lb/ft³ |
| Serbian sprucePicea omorika | 449 lbf* | 26.7 lb/ft³ |
| Sitka sprucePicea sitchensis | 510 lbf | 28.0 lb/ft³ |
| White sprucePicea glauca | 410 lbf | 25.2 lb/ft³ |