Woods sold under several trade names often come from one genus. These 6 share the genus Pseudotsuga, so they are close relatives and frequent substitutes for each other.

4 of 6 carry a published Janka test.

WoodJankaDensity
Bigcone Douglas-firPseudotsuga macrocarpa645 lbf*33.9 lb/ft³
Coast Douglas-firPseudotsuga menziesii710 lbf33.6 lb/ft³
Douglas-firPseudotsuga menziesii645 lbf*33.9 lb/ft³
Interior North Douglas-firPseudotsuga menziesii600 lbf33.6 lb/ft³
Interior South Douglas-firPseudotsuga menziesii510 lbf32.2 lb/ft³
Interior West Douglas-firPseudotsuga menziesii660 lbf35.0 lb/ft³