genus
Shorea
Woods sold under several trade names often come from one genus. These 5 share the genus Shorea, so they are close relatives and frequent substitutes for each other.
5 of 5 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Dark red merantiShorea spp. | 780 lbf | 53.0 lb/ft³ |
| Light red merantiShorea spp. | 460 lbf | 25.1 lb/ft³ |
| ShoreaShorea spp., bullau group | 1,780 lbf | 53.3 lb/ft³ |
| White merantiShorea spp. | 1,140 lbf | 42.1 lb/ft³ |
| Yellow merantiShorea spp. | 770 lbf | 34.7 lb/ft³ |