genus
Thuja
Woods sold under several trade names often come from one genus. These 2 share the genus Thuja, so they are close relatives and frequent substitutes for each other.
2 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Northern white cedarThuja occidentalis | 320 lbf | 21.7 lb/ft³ |
| Western redcedarThuja plicata | 350 lbf | 22.3 lb/ft³ |