All wood species
1,785 species. 571 carry a published Janka test. A species with no test says so.
1,785 matching species · Estimates are marked with an asterisk. Images may show a related species; see credits.
| Wood | Region | Wood type | Janka hardness | Density |
|---|---|---|---|---|
| Tropical America | hardwood | 2,700 lbf | 55.0 lb/ft³ | |
| Tropical America | hardwood | 700 lbf | 36.0 lb/ft³ | |
| Range not recorded | hardwood | 1,475 lbf* | 46.4 lb/ft³* | |
| Tropical America | hardwood | 379 lbf | 32.5 lb/ft³ | |
Letterwood Piratlnera guianensis | Tropical America | hardwood | 4,669 lbf* | 74.0 lb/ft³ |
| Range not recorded | hardwood | 451 lbf* | 26.7 lb/ft³* | |
Leyland cypress Cupressocyparis leylandii | Range not recorded | softwood | 554 lbf* | 30.7 lb/ft³* |
| Range not recorded | hardwood | 1,103 lbf* | 40.5 lb/ft³* | |
| Asia | hardwood | 460 lbf | 25.1 lb/ft³* | |
| Range not recorded | hardwood | 5,728 lbf* | 87.1 lb/ft³* | |
| Tropical America | hardwood | 4,500 lbf | 80.0 lb/ft³ | |
| Range not recorded | hardwood | 1,363 lbf* | 44.7 lb/ft³* | |
| Africa | hardwood | 490 lbf | 34.0 lb/ft³ | |
| Range not recorded | softwood | 469 lbf* | 27.5 lb/ft³* | |
| Range not recorded | hardwood | 915 lbf* | 37.1 lb/ft³* | |
| Range not recorded | hardwood | 1,658 lbf* | 48.9 lb/ft³* | |
| Range not recorded | hardwood | 1,923 lbf* | 52.4 lb/ft³* | |
| Tropical America | hardwood | 860 lbf | 36.0 lb/ft³ | |
| Range not recorded | hardwood | 423 lbf* | 26.0 lb/ft³* | |
Little silverbell Halesia parviflora | Range not recorded | hardwood | 641 lbf* | 31.5 lb/ft³* |
| Range not recorded | hardwood | 1,054 lbf* | 39.6 lb/ft³* | |
| Range not recorded | hardwood | 344 lbf* | 23.5 lb/ft³* | |
| North America | hardwood | 2,712 lbf* | 61.6 lb/ft³ | |
| North America | softwood | 690 lbf | 35.6 lb/ft³ | |
| Range not recorded | hardwood | 915 lbf* | 37.1 lb/ft³* | |
| Range not recorded | hardwood | 679 lbf* | 32.3 lb/ft³* | |
| North America | softwood | 480 lbf | 28.7 lb/ft³ | |
| Range not recorded | hardwood | 791 lbf* | 34.7 lb/ft³* | |
| Tropical America | hardwood | 1,430 lbf | 43.0 lb/ft³ | |
| Range not recorded | hardwood | 1,203 lbf* | 42.1 lb/ft³* | |
| North America | softwood | 870 lbf | 41.3 lb/ft³ | |
| Africa | hardwood | 1,658 lbf* | 48.9 lb/ft³* | |
| Range not recorded | hardwood | 2,448 lbf* | 58.7 lb/ft³* | |
| Tropical America | hardwood | 1,198 lbf | 38.4 lb/ft³ | |
Louro Anaueria brasiliensis = Beilschmiedia brasiliensis | Tropical America | hardwood | 1,257 lbf | 45.6 lb/ft³ |
| Tropical America | hardwood | 2,019 lbf | 57.7 lb/ft³* | |
| Tropical America | hardwood | 2,169 lbf | 61.3 lb/ft³* | |
| Tropical America | hardwood | 1,135 lbf | 42.1 lb/ft³* | |
| Tropical America | hardwood | 1,010 lbf | 42.1 lb/ft³* | |
| Tropical America | hardwood | 1,063 lbf | 36.2 lb/ft³ | |
| Tropical America | hardwood | 756 lbf | 42.1 lb/ft³* | |
| Range not recorded | hardwood | 1,363 lbf* | 44.7 lb/ft³* | |
| Range not recorded | hardwood | 1,103 lbf* | 40.5 lb/ft³* | |
| Range not recorded | hardwood | 3,241 lbf* | 66.9 lb/ft³* | |
| Range not recorded | hardwood | 915 lbf* | 37.1 lb/ft³* | |
| Range not recorded | hardwood | 3,147 lbf* | 65.9 lb/ft³* | |
| Range not recorded | hardwood | 1,538 lbf* | 47.3 lb/ft³* | |
| Range not recorded | hardwood | 2,064 lbf* | 54.2 lb/ft³* | |
| Tropical America | hardwood | 3,228 lbf | 66.8 lb/ft³ | |
| Tropical America | hardwood | 3,047 lbf | 66.8 lb/ft³ | |
| Tropical America | hardwood | 2,725 lbf | 61.8 lb/ft³ | |
| Tropical America | hardwood | 3,150 lbf | 64.0 lb/ft³ | |
| Asia | hardwood | 630 lbf | 32.0 lb/ft³ | |
| Tropical America | hardwood | 3,153 lbf | 58.7 lb/ft³ | |
| Africa | hardwood | 1,370 lbf | 43.0 lb/ft³ | |
| Range not recorded | hardwood | 1,475 lbf* | 46.4 lb/ft³* | |
| Asia | hardwood | 462 lbf | 25.0 lb/ft³ | |
| Range not recorded | hardwood | 451 lbf* | 26.7 lb/ft³* | |
| Tropical America | hardwood | 1,090 lbf | 39.0 lb/ft³ | |
| Range not recorded | hardwood | 276 lbf* | 21.2 lb/ft³* | |
| Range not recorded | hardwood | 832 lbf* | 35.5 lb/ft³* | |
| Range not recorded | hardwood | 1,007 lbf* | 38.8 lb/ft³* | |
| Tropical America | hardwood | 960 lbf* | 37.0 lb/ft³ | |
| Range not recorded | hardwood | 2,963 lbf* | 64.1 lb/ft³* | |
| Africa | hardwood | 1,110 lbf | 42.0 lb/ft³ | |
| Range not recorded | hardwood | 2,210 lbf* | 55.9 lb/ft³* | |
| Range not recorded | hardwood | 1,007 lbf* | 38.8 lb/ft³* | |
| Range not recorded | hardwood | 1,309 lbf* | 43.8 lb/ft³* | |
| Range not recorded | hardwood | 1,363 lbf* | 44.7 lb/ft³* | |
| Range not recorded | hardwood | 2,867 lbf* | 63.1 lb/ft³* | |
| Tropical America | hardwood | 791 lbf | 37.5 lb/ft³ | |
| Range not recorded | hardwood | 1,852 lbf* | 51.5 lb/ft³* | |
| Range not recorded | hardwood | 1,923 lbf* | 52.4 lb/ft³* | |
| Range not recorded | hardwood | 2,867 lbf* | 63.1 lb/ft³* | |
| Tropical America | hardwood | 3,480 lbf | 46.2 lb/ft³ | |
| Range not recorded | hardwood | 960 lbf* | 38.0 lb/ft³* | |
| Tropical America | hardwood | 1,351 lbf | 42.0 lb/ft³ | |
| Tropical America | hardwood | 1,071 lbf | 44.7 lb/ft³* | |
| Tropical America | hardwood | 2,165 lbf | 58.7 lb/ft³* | |
| Tropical America | hardwood | 1,363 lbf* | 44.7 lb/ft³* | |
| Range not recorded | hardwood | 3,965 lbf* | 73.4 lb/ft³* | |
| Tropical America | hardwood | 2,760 lbf | 67.0 lb/ft³ | |
| Range not recorded | hardwood | 2,607 lbf* | 60.4 lb/ft³* | |
| Asia | hardwood | 1,000 lbf | 40.0 lb/ft³ | |
| Range not recorded | hardwood | 1,103 lbf* | 40.5 lb/ft³* | |
| Range not recorded | hardwood | 2,530 lbf* | 59.6 lb/ft³* | |
| Range not recorded | hardwood | 1,309 lbf* | 43.8 lb/ft³* | |
| Range not recorded | hardwood | 1,923 lbf* | 52.4 lb/ft³* | |
| Tropical America | hardwood | 1,120 lbf | 44.0 lb/ft³ | |
| Africa | hardwood | 1,290 lbf | 42.0 lb/ft³ | |
| Range not recorded | hardwood | 1,309 lbf* | 43.8 lb/ft³* | |
| Range not recorded | hardwood | 1,203 lbf* | 42.1 lb/ft³* | |
| Range not recorded | hardwood | 542 lbf* | 29.1 lb/ft³* | |
Maouli Trichospermum richii | Range not recorded | hardwood | 395 lbf* | 25.1 lb/ft³* |
| Tropical America | hardwood | 1,746 lbf | 48.7 lb/ft³ | |
| Range not recorded | hardwood | 1,152 lbf* | 41.3 lb/ft³* | |
Maria-preta Zizyphus cinnamomum = Zizyphus itacaiunensis | Tropical America | hardwood | 3,331 lbf | 60.6 lb/ft³ |
| Range not recorded | hardwood | 1,475 lbf* | 46.4 lb/ft³* | |
Marishballi Lincania spp. | Tropical America | hardwood | 3,570 lbf | 62.0 lb/ft³ |
| Range not recorded | softwood | 766 lbf* | 38.0 lb/ft³* |