Wood Record

genus

Tsuga

Woods sold under several trade names often come from one genus. These 4 share the genus Tsuga, so they are close relatives and frequent substitutes for each other.

3 of 4 carry a published Janka test.

WoodJankaDensity
Carolina hemlockTsuga caroliniana554 lbf*30.7 lb/ft³
Eastern hemlockTsuga canadensis500 lbf28.0 lb/ft³
Mountain hemlockTsuga mertensiana680 lbf31.5 lb/ft³
Western hemlockTsuga heterophylla540 lbf31.5 lb/ft³