All wood species
1,785 species. 571 carry a published Janka test. A species with no test says so.
1,785 matching species · Estimates are marked with an asterisk. Images may show a related species; see credits.
| Wood | Region | Wood type | Janka hardness | Density |
|---|---|---|---|---|
| North America | hardwood | 1,277 lbf* | 43.3 lb/ft³ | |
| Range not recorded | hardwood | 395 lbf* | 25.1 lb/ft³* | |
| North America | hardwood | 1,190 lbf | 44.1 lb/ft³ | |
| North America | hardwood | 880 lbf | 35.0 lb/ft³ | |
Waterlocust Gleditsia aquatica François André Michaux (book author), Augustus Lucas Hillhouse (translator), iii · Public domain | Range not recorded | hardwood | 1,475 lbf* | 46.4 lb/ft³* |
| Range not recorded | hardwood | 915 lbf* | 37.1 lb/ft³* | |
| Africa | hardwood | 590 lbf | 25.0 lb/ft³ | |
| Tropical America | hardwood | 2,064 lbf* | 53.0 lb/ft³ | |
| Range not recorded | hardwood | 1,923 lbf* | 52.4 lb/ft³* | |
West Indian false box Gyminda latifolia | Range not recorded | hardwood | 2,867 lbf* | 63.1 lb/ft³* |
| Tropical America | hardwood | 2,830 lbf | 62.0 lb/ft³ | |
| Range not recorded | hardwood | 1,419 lbf* | 45.5 lb/ft³* | |
| Range not recorded | hardwood | 2,448 lbf* | 58.7 lb/ft³* | |
| Range not recorded | hardwood | 1,475 lbf* | 46.4 lb/ft³* | |
| Range not recorded | hardwood | 2,287 lbf* | 56.9 lb/ft³* | |
| North America | softwood | 540 lbf | 31.5 lb/ft³ | |
| Range not recorded | softwood | 645 lbf* | 33.9 lb/ft³* | |
| North America | softwood | 830 lbf | 36.3 lb/ft³ | |
| Range not recorded | hardwood | 1,054 lbf* | 39.6 lb/ft³* | |
| North America | softwood | 350 lbf | 22.3 lb/ft³ | |
| North America | softwood | 420 lbf | 26.6 lb/ft³ | |
White alder Alnus rhombifolia US NPS Santa Monica Mountains National Recreation Area [2] · Public domain | Range not recorded | hardwood | 479 lbf* | 27.5 lb/ft³* |
| North America | hardwood | 1,320 lbf | 42.0 lb/ft³ | |
| Asia | hardwood | 1,070 lbf | 40.0 lb/ft³ | |
| Range not recorded | hardwood | 1,152 lbf* | 41.3 lb/ft³* | |
| Asia | hardwood | 1,190 lbf | 43.0 lb/ft³ | |
| Range not recorded | hardwood | 2,210 lbf* | 55.9 lb/ft³* | |
White Cypress-Pine Callitris glauca | Oceania | softwood | 1,375 lbf | 42.0 lb/ft³ |
| North America | softwood | 480 lbf | 27.3 lb/ft³ | |
| Range not recorded | hardwood | 1,990 lbf* | 53.3 lb/ft³* | |
| Range not recorded | hardwood | 2,692 lbf* | 61.3 lb/ft³* | |
| Asia | hardwood | 690 lbf | 33.0 lb/ft³ | |
| Range not recorded | hardwood | 1,658 lbf* | 48.9 lb/ft³* | |
| Range not recorded | hardwood | 1,363 lbf* | 44.7 lb/ft³* | |
| Asia | hardwood | 1,140 lbf | 42.1 lb/ft³* | |
| Range not recorded | hardwood | 1,363 lbf* | 44.7 lb/ft³* | |
White oak Quercus alba | North America | hardwood | 1,360 lbf | 47.6 lb/ft³ |
| Range not recorded | hardwood | 832 lbf* | 35.5 lb/ft³* | |
| Range not recorded | hardwood | 1,658 lbf* | 48.9 lb/ft³* | |
White rosewood Chionanthus domingensis | Range not recorded | hardwood | 2,963 lbf* | 64.1 lb/ft³* |
| Asia | hardwood | 838 lbf | 33.0 lb/ft³ | |
| North America | softwood | 410 lbf | 25.2 lb/ft³ | |
| Range not recorded | hardwood | 2,064 lbf* | 54.2 lb/ft³* | |
| Range not recorded | hardwood | 451 lbf* | 26.7 lb/ft³* | |
| Range not recorded | softwood | 599 lbf* | 32.3 lb/ft³* | |
| Range not recorded | hardwood | 1,309 lbf* | 43.8 lb/ft³* | |
| Range not recorded | hardwood | 1,363 lbf* | 44.7 lb/ft³* | |
| Range not recorded | hardwood | 832 lbf* | 35.5 lb/ft³* | |
| Europe | hardwood | 1,152 lbf* | 41.3 lb/ft³* | |
| Range not recorded | hardwood | 714 lbf* | 33.1 lb/ft³* | |
| Range not recorded | hardwood | 3,749 lbf* | 71.5 lb/ft³* | |
| Range not recorded | hardwood | 2,064 lbf* | 54.2 lb/ft³* | |
| Range not recorded | hardwood | 3,147 lbf* | 65.9 lb/ft³* | |
| Range not recorded | hardwood | 1,852 lbf* | 51.5 lb/ft³* | |
| Range not recorded | hardwood | 1,788 lbf* | 50.7 lb/ft³* | |
| Range not recorded | hardwood | 276 lbf* | 21.2 lb/ft³* | |
| Range not recorded | hardwood | 2,867 lbf* | 63.1 lb/ft³* | |
| North America | hardwood | 1,460 lbf | 48.3 lb/ft³ | |
| North America | hardwood | 1,475 lbf* | 46.4 lb/ft³* | |
| Range not recorded | hardwood | 818 lbf* | 35.2 lb/ft³* | |
| Range not recorded | hardwood | 1,788 lbf* | 50.7 lb/ft³* | |
| Range not recorded | hardwood | 1,363 lbf* | 44.7 lb/ft³* | |
| Range not recorded | hardwood | 1,475 lbf* | 46.4 lb/ft³* | |
| Tropical America | hardwood | 1,071 lbf | 39.4 lb/ft³* | |
| Range not recorded | hardwood | 1,658 lbf* | 48.9 lb/ft³* | |
| Range not recorded | hardwood | 3,147 lbf* | 65.9 lb/ft³* | |
| Range not recorded | hardwood | 1,054 lbf* | 39.6 lb/ft³* | |
| North America | hardwood | 1,260 lbf | 43.3 lb/ft³ | |
| North America | hardwood | 369 lbf* | 24.3 lb/ft³* | |
Yellow cedar Chamaecyparis nootkatensis | North America | softwood | 580 lbf | 30.8 lb/ft³ |
| Range not recorded | hardwood | 1,538 lbf* | 47.3 lb/ft³* | |
| Asia | hardwood | 770 lbf | 34.7 lb/ft³* | |
| Tropical America | hardwood | 1,220 lbf | 47.0 lb/ft³ | |
| Africa | hardwood | 1,120 lbf | 48.0 lb/ft³ | |
| Range not recorded | hardwood | 915 lbf* | 37.1 lb/ft³* | |
| Range not recorded | hardwood | 451 lbf* | 26.7 lb/ft³* | |
| North America | hardwood | 540 lbf | 29.3 lb/ft³ | |
| Range not recorded | hardwood | 1,538 lbf* | 47.3 lb/ft³* | |
| Range not recorded | hardwood | 714 lbf* | 33.1 lb/ft³* | |
| Tropical America | hardwood | 605 lbf | 36.0 lb/ft³ | |
| Range not recorded | softwood | 898 lbf* | 42.1 lb/ft³* | |
| North America | softwood | 420 lbf | 24.5 lb/ft³ | |
| Range not recorded | hardwood | 1,255 lbf* | 43.0 lb/ft³* | |
| Africa | hardwood | 2,139 lbf* | 53.0 lb/ft³ | |
| Tropical America | hardwood | 2,530 lbf* | 59.6 lb/ft³* |