Wood Record

All wood species

1,785 species. 571 carry a published Janka test. A species with no test says so.

1,785 matching species · Estimates are marked with an asterisk. Images may show a related species; see credits.

Wood species and selected properties
WoodRegionWood typeJanka hardnessDensity
Guachapele

Pseudosamanea guachapele

Tropical Americahardwood1,255 lbf*41.0 lb/ft³
Guadeloupe marlberry

Ardisia obovata

Range not recordedhardwood1,475 lbf*46.4 lb/ft³*
Guanacaste

Enterolobium cyclocarpum

Genus image · Cirad · Public domain
Tropical Americahardwood520 lbf26.0 lb/ft³
Guarea

Guarea cedrata

Cirad · Public domain
Africahardwood1,000 lbf36.0 lb/ft³
Guariúba

Clarisia racemosa

Cirad · Public domain
Tropical Americahardwood1,380 lbf41.2 lb/ft³
Range not recordedhardwood1,598 lbf*48.1 lb/ft³*
Guava

Psidium guajava

Cirad · Public domain
Range not recordedhardwood1,475 lbf*46.4 lb/ft³*
Guavaberry

Myrciaria floribunda

Cirad · Public domain
Range not recordedhardwood2,692 lbf*61.3 lb/ft³*
Gubas

Endospermum spp.

Genus image · Cirad · Public domain
Asiahardwood509 lbf*30.0 lb/ft³
Guest tree

Kleinhovia hospita

J.M.Garg · CC BY-SA 3.0
Range not recordedhardwood641 lbf*31.5 lb/ft³*
Guiana plum

Drypetes lateriflora

Genus image · Cirad · Public domain
Range not recordedhardwood2,287 lbf*56.9 lb/ft³*
Gulf graytwig

Schoepfia schreberi

Alison Northup · CC BY
Range not recordedhardwood1,852 lbf*51.5 lb/ft³*
Gulos

Cynometra ramiflora

Genus image · Cirad · Public domain
Range not recordedhardwood2,287 lbf*56.9 lb/ft³*
Gumbo-Limbo

Bursera simaruba

Genus image · Cirad · Public domain
Tropical Americahardwood395 lbf*25.1 lb/ft³*
Guyanese pepper

Piper glabrescens

Genus image · Cirad · Public domain
Range not recordedhardwood423 lbf*26.0 lb/ft³*
Guyanese wild coffee

Casearia guianensis

Genus image · Cirad · Public domain
Range not recordedhardwood1,990 lbf*53.3 lb/ft³*
Ha a

Antidesma platyphyllum

Genus image · Cirad · Public domain
Range not recordedhardwood1,923 lbf*52.4 lb/ft³*
Hackberry

Celtis occidentalis

Genus image · Cirad · Public domain
North Americahardwood880 lbf37.1 lb/ft³
Haiari

Alexa imperatricis

Cirad · Public domain
Tropical Americahardwood690 lbf38.4 lb/ft³*
Haitian catalpa

Catalpa longissima

Genus image · Brya · CC BY-SA 4.0
Range not recordedhardwood1,007 lbf*38.8 lb/ft³*
Haldu

Adina cordifolia

Cirad · Public domain
Asiahardwood1,140 lbf44.0 lb/ft³
Hammock velvetseed

Guettarda elliptica

Genus image · Cirad · Public domain
Range not recordedhardwood2,064 lbf*54.2 lb/ft³*
Haplolobus floribundus

Haplolobus floribundus

Range not recordedhardwood1,725 lbf*49.9 lb/ft³*
Hapuu

Cibotium glaucum

Hermann Luyken · CC0
Range not recordedhardwood255 lbf*20.5 lb/ft³*
Range not recordedhardwood255 lbf*20.5 lb/ft³*
Range not recordedhardwood1,725 lbf*49.9 lb/ft³*
Haujillo

Havardia pallens

Range not recordedhardwood2,287 lbf*56.9 lb/ft³*
Havard oak

Quercus havardii

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Hawaii holly

Ilex anomala

Cirad · Public domain
Range not recordedhardwood791 lbf*34.7 lb/ft³*
Hawaii roughbush

Streblus pendulinus

Genus image · Cirad · Public domain
Range not recordedhardwood1,788 lbf*50.7 lb/ft³*
Haya

Oxandra laurifolia

Genus image · Cirad · Public domain
Range not recordedhardwood1,725 lbf*49.9 lb/ft³*
Haya blanca

Guatteria caribaea

Cirad · Public domain
Range not recordedhardwood1,203 lbf*42.1 lb/ft³*
Haya minga

Guatteria blainii

Genus image · Cirad · Public domain
Range not recordedhardwood1,598 lbf*48.1 lb/ft³*
Range not recordedhardwood479 lbf*27.5 lb/ft³*
Hazel sterculia

Sterculia foetida

Genus image · Cirad · Public domain
Range not recordedhardwood875 lbf*36.3 lb/ft³*
Hedge maple

Acer campestre

Genus image · Cirad · Public domain
Range not recordedhardwood832 lbf*35.5 lb/ft³*
Hercules' club

Zanthoxylum clava-herculis

Genus image · Cirad · Public domain
Range not recordedhardwood1,203 lbf*42.1 lb/ft³*
Range not recordedhardwood451 lbf*26.7 lb/ft³*
Higo

Ficus virens

Genus image · Cirad · Public domain
Range not recordedhardwood608 lbf*30.7 lb/ft³*
Higuerillo

Vitex divaricata

Cirad · Public domain
Range not recordedhardwood1,309 lbf*43.8 lb/ft³*
Higuillo de hoja menuda

Piper aduncum

Genus image · Cirad · Public domain
Range not recordedhardwood573 lbf*29.8 lb/ft³*
Higuillo de limon

Piper amalago

Genus image · Cirad · Public domain
Range not recordedhardwood1,152 lbf*41.3 lb/ft³*
Range not recordedhardwood1,007 lbf*38.8 lb/ft³*
Hinchahuevos

Sapium laurifolium

Range not recordedhardwood542 lbf*29.1 lb/ft³*
Hinoki

Chamaecyparis obtusa

Σ64 · CC BY 3.0
Asiasoftwood599 lbf*32.3 lb/ft³*
Hoja menuda

Siphoneugena densiflora

João Medeiros · CC BY
Range not recordedhardwood2,779 lbf*62.2 lb/ft³*
Holio

Cryptocarya mannii

Genus image · Cirad · Public domain
Range not recordedhardwood1,007 lbf*38.8 lb/ft³*
Holly oak

Quercus ilex

Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Holywood

Guaiacum sanctum

Mangostar · CC BY-SA 3.0
Range not recordedhardwood5,728 lbf*87.1 lb/ft³*
Honduras Rosewood

Dalbergia stevensonii

Genus image · Cirad · Public domain
Tropical Americahardwood3,097 lbf*63.0 lb/ft³
Honey mesquite

Prosopis glandulosa

Genus image · Abestrobi · Public domain
North Americahardwood2,779 lbf*62.2 lb/ft³*
Honeylocust

Gleditsia triacanthos

Roger Culos · CC BY-SA 3.0
North Americahardwood1,580 lbf46.4 lb/ft³*
Hoop-Pine

Araucaria spp.

Genus image · Cirad · Public domain
Oceaniasoftwood576 lbf*31.0 lb/ft³
Range not recordedhardwood369 lbf*24.3 lb/ft³*
Range not recordedhardwood216 lbf*19.0 lb/ft³*
Houka, calabash

Crescentia alata

Francisco Manuel Blanco (O.S.A.) · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Huon pine

Lagarostrobos franklinii

Matt Berger · CC BY 4.0
Oceaniasoftwood926 lbf*43.0 lb/ft³*
Hura

Hura crepitans

Cirad · Public domain
Tropical Americahardwood550 lbf30.0 lb/ft³
Icaco coco plum

Chrysobalanus icaco

Cirad · Public domain
Range not recordedhardwood2,210 lbf*55.9 lb/ft³*
Ice cream bean

Inga edulis

Cirad · Public domain
Range not recordedhardwood1,054 lbf*39.6 lb/ft³*
Idígbo

Terminalia ivorensis

Cirad · Public domain
Africahardwood845 lbf32.0 lb/ft³
Ifi

Inocarpus fagifer

Cirad · Public domain
Range not recordedhardwood960 lbf*38.0 lb/ft³*
Ifilele

Intsia bijuga

Cirad · Public domain
Range not recordedhardwood1,788 lbf*50.7 lb/ft³*
Ilang-ilang

Cananga odorata

Cirad · Public domain
Range not recordedhardwood509 lbf*28.2 lb/ft³*
Ilomba

Pycnanthus angolensis

Cirad · Public domain
Africahardwood610 lbf29.8 lb/ft³*
Imbuia

Phoebe porosa

Cirad · Public domain
Tropical Americahardwood950 lbf40.0 lb/ft³
North Americasoftwood470 lbf25.8 lb/ft³
Indian Almond Wood

Terminalia catappa

Cirad · Public domain
Asiahardwood1,030 lbf*40.0 lb/ft³
Indian banyan

Ficus benghalensis

Genus image · Cirad · Public domain
Range not recordedhardwood791 lbf*34.7 lb/ft³*
Indian jujube

Ziziphus mauritiana

Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Indian Laurel

Terminalia tomentosa complex

Genus image · Cirad · Public domain
Asiahardwood2,220 lbf54.0 lb/ft³
Indian longleaf pine

Pinus roxburghii

Genus image · Cirad · Public domain
Range not recordedsoftwood668 lbf*34.7 lb/ft³*
Indian mulberry

Morinda citrifolia

Cirad · Public domain
Range not recordedhardwood791 lbf*34.7 lb/ft³*
Indian rosewood

Dalbergia latifolia

Cirad · Public domain
Asiahardwood3,170 lbf53.0 lb/ft³
Indian rosewood

Dalbergia sissoo

Cirad · Public domain
Range not recordedhardwood1,598 lbf*48.1 lb/ft³*
Indian rubberplant

Ficus elastica

Cirad · Public domain
Range not recordedhardwood960 lbf*38.0 lb/ft³*
Range not recordedhardwood451 lbf*26.7 lb/ft³*
Range not recordedhardwood542 lbf*29.1 lb/ft³*
Ingá

Inga paraensis

Genus image · Cirad · Public domain
Tropical Americahardwood3,064 lbf65.9 lb/ft³*
Ingá

Inga sp

Genus image · Cirad · Public domain
Tropical Americahardwood2,846 lbf68.7 lb/ft³*
Ingá / ingá xixi

Inga alba

Cirad · Public domain
Tropical Americahardwood1,418 lbf48.1 lb/ft³*
Inga nobilis

Inga nobilis

Genus image · Cirad · Public domain
Range not recordedhardwood1,363 lbf*44.7 lb/ft³*
Inga-de-porco

Albizia pedicellaris = Macrosamanea pedicellaris

Cirad · Public domain
Tropical Americahardwood955 lbf38.1 lb/ft³
Inkwood

Hypelate trifoliata

Homer Edward Price · CC BY 2.0
Range not recordedhardwood2,963 lbf*64.1 lb/ft³*
Interior live oak

Quercus wislizeni

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Interior North Douglas-fir

Pseudotsuga menziesii

Cirad · Public domain
North Americasoftwood600 lbf33.6 lb/ft³
Interior South Douglas-fir

Pseudotsuga menziesii

Cirad · Public domain
North Americasoftwood510 lbf32.2 lb/ft³
Interior West Douglas-fir

Pseudotsuga menziesii

Cirad · Public domain
North Americasoftwood660 lbf35.0 lb/ft³
Ipe

Tabebuia spp., lapacho group

Genus image · Cirad · Public domain
Tropical Americahardwood3,680 lbf70.0 lb/ft³
Ipê

Handroanthus serratifolius = Tabebuia serratifolia

Cirad · Public domain
Tropical Americahardwood3,100 lbf72.5 lb/ft³*
Ipê

Tabebuia sp

Genus image · Cirad · Public domain
Tropical Americahardwood1,280 lbf63.7 lb/ft³
Ipê-amarelo

Handroanthus incanus = Tabebuia cf incana

Genus image · Cirad · Public domain
Tropical Americahardwood3,147 lbf*65.5 lb/ft³
Iroko

Chlorophora spp.

Genus image · Cirad · Public domain
Africahardwood1,260 lbf43.0 lb/ft³
Range not recordedhardwood479 lbf*27.5 lb/ft³*
Range not recordedsoftwood740 lbf*37.1 lb/ft³*
Italian stone pine

Pinus pinea

Genus image · Cirad · Public domain
Range not recordedsoftwood599 lbf*32.3 lb/ft³*
Itaúba

Mezilaurus lindaviana

Cirad · Public domain
Tropical Americahardwood992 lbf53.3 lb/ft³*
Itaúba / itaúba-vermelha

Mezilaurus itauba

Genus image · Cirad · Public domain
Tropical Americahardwood1,262 lbf54.2 lb/ft³*
Izombé

Testulea gabonensis

Cirad · Public domain
Africahardwood1,475 lbf*46.0 lb/ft³
Jack pine

Pinus banksiana

Genus image · Cirad · Public domain
North Americasoftwood570 lbf30.1 lb/ft³