Wood Record

family

Pinaceae

The family Pinaceae supplies 95 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

38 of 95 carry a published Janka test.

WoodJankaDensity
Aleppo pinePinus halepensis599 lbf*32.3 lb/ft³
Apache pinePinus engelmannii599 lbf*32.3 lb/ft³
Arizona pinePinus arizonica599 lbf*32.3 lb/ft³
Atlas cedarCedrus atlantica554 lbf*30.7 lb/ft³
Austrian pinePinus nigra599 lbf*32.3 lb/ft³
Balsam firAbies balsamea380 lbf24.5 lb/ft³
Benguet PinePinus insularis605 lbf35.0 lb/ft³
Bigcone Douglas-firPseudotsuga macrocarpa645 lbf*33.9 lb/ft³
Bishop pinePinus muricata645 lbf*33.9 lb/ft³
Black sprucePicea mariana530 lbf29.3 lb/ft³
Blue sprucePicea pungens449 lbf*26.7 lb/ft³
Border pinyonPinus discolor599 lbf*32.3 lb/ft³
Brewer sprucePicea breweriana449 lbf*26.7 lb/ft³
Bunge's pinePinus bungeana599 lbf*32.3 lb/ft³
California red firAbies magnifica500 lbf26.6 lb/ft³
Canary Island pinePinus canariensis599 lbf*32.3 lb/ft³
Caribbean pinePinus caribaea1,240 lbf38.0 lb/ft³
Carolina hemlockTsuga caroliniana554 lbf*30.7 lb/ft³
Cedar of LebanonCedrus libani692 lbf*35.5 lb/ft³
Chihuahuan pinePinus leiophylla599 lbf*32.3 lb/ft³
Chinese red pinePinus massoniana740 lbf*37.1 lb/ft³
Coast Douglas-firPseudotsuga menziesii710 lbf33.6 lb/ft³
Common or two-needle pinyonPinus edulis766 lbf*38.0 lb/ft³
Coulter pinePinus coulteri599 lbf*32.3 lb/ft³
Deodar cedarCedrus deodara844 lbf*40.5 lb/ft³
Douglas-firPseudotsuga menziesii645 lbf*33.9 lb/ft³
Eastern hemlockTsuga canadensis500 lbf28.0 lb/ft³
Eastern white pinePinus strobus380 lbf24.5 lb/ft³
Engelmann sprucePicea engelmannii390 lbf24.5 lb/ft³
European larchLarix decidua740 lbf*37.1 lb/ft³
Five-needle pinePinus parviflora599 lbf*32.3 lb/ft³
Four-leaf or Parry pinyon pinePinus quadrifolia599 lbf*32.3 lb/ft³
Foxtail pinePinus balfouriana599 lbf*32.3 lb/ft³
Fraser firAbies fraseri449 lbf*26.7 lb/ft³
Grand firAbies grandis490 lbf25.8 lb/ft³
Gray or California foothill pinePinus sabiniana532 lbf*29.8 lb/ft³
Great Basin bristlecone pinePinus longaeva599 lbf*32.3 lb/ft³
Indian longleaf pinePinus roxburghii668 lbf*34.7 lb/ft³
Interior North Douglas-firPseudotsuga menziesii600 lbf33.6 lb/ft³
Interior South Douglas-firPseudotsuga menziesii510 lbf32.2 lb/ft³
Interior West Douglas-firPseudotsuga menziesii660 lbf35.0 lb/ft³
Italian stone pinePinus pinea599 lbf*32.3 lb/ft³
Jack pinePinus banksiana570 lbf30.1 lb/ft³
Japanese black pinePinus thunbergii599 lbf*32.3 lb/ft³
Japanese red pinePinus densiflora599 lbf*32.3 lb/ft³
Jeffrey pinePinus jeffreyi469 lbf*27.5 lb/ft³
Knobcone pinePinus attenuata511 lbf*29.1 lb/ft³
Limber pinePinus flexilis469 lbf*27.5 lb/ft³
Loblolly pinePinus taeda690 lbf35.6 lb/ft³
Lodgepole pinePinus contorta480 lbf28.7 lb/ft³
Longleaf pinePinus palustris870 lbf41.3 lb/ft³
Maritime pinePinus pinaster766 lbf*38.0 lb/ft³
Merkus PinePinus merkusii620 lbf43.0 lb/ft³
Mexican pinyon pinePinus cembroides599 lbf*32.3 lb/ft³
Mountain hemlockTsuga mertensiana680 lbf31.5 lb/ft³
Noble firAbies procera410 lbf27.3 lb/ft³
Norway sprucePicea abies449 lbf*26.7 lb/ft³
Ocote pinePinus oocarpa910 lbf41.0 lb/ft³
Pacific silver firAbies amabilis430 lbf30.1 lb/ft³
Papershell pinyon pinePinus remota599 lbf*32.3 lb/ft³
Patula PinePinus patula (plantation)645 lbf*34.0 lb/ft³
Pitch pinePinus rigida717 lbf*36.3 lb/ft³
Pond pinePinus serotina803 lbf*39.1 lb/ft³
Ponderosa pinePinus ponderosa460 lbf28.0 lb/ft³
Radiata pinePinus radiata750 lbf31.5 lb/ft³
Red pinePinus resinosa560 lbf32.2 lb/ft³
Red sprucePicea rubens530 lbf28.0 lb/ft³
Rocky Mountain bristlecone pinePinus aristata599 lbf*32.3 lb/ft³
Sakhalin sprucePicea glehnii449 lbf*26.7 lb/ft³
Sand pinePinus clausa635 lbf*33.6 lb/ft³
Santa Lucia or bristlecone firAbies bracteata449 lbf*26.7 lb/ft³
Scots pinePinus sylvestris621 lbf*33.1 lb/ft³
Serbian sprucePicea omorika449 lbf*26.7 lb/ft³
Shasta red firAbies shastensis449 lbf*26.7 lb/ft³
Shortleaf pinePinus echinata690 lbf35.6 lb/ft³
Silver firAbies alba576 lbf*31.5 lb/ft³
Singleleaf pinyonPinus monophylla599 lbf*32.3 lb/ft³
Sitka sprucePicea sitchensis510 lbf28.0 lb/ft³
Slash pinePinus elliottii869 lbf*41.3 lb/ft³
Southwestern white pinePinus strobiformis599 lbf*32.3 lb/ft³
Spruce pinePinus glabra660 lbf30.8 lb/ft³
Subalpine firAbies lasiocarpa350 lbf22.3 lb/ft³
Subalpine larchLarix lyallii740 lbf*37.1 lb/ft³
Sugar pinePinus lambertiana380 lbf25.2 lb/ft³
Table Mountain pinePinus pungens740 lbf*37.1 lb/ft³
TamarackLarix laricina590 lbf37.1 lb/ft³
Torrey pinePinus torreyana599 lbf*32.3 lb/ft³
Virginia pinePinus virginiana740 lbf33.6 lb/ft³
Washoe pinePinus washoensis599 lbf*32.3 lb/ft³
Western hemlockTsuga heterophylla540 lbf31.5 lb/ft³
Western larchLarix occidentalis830 lbf36.3 lb/ft³
Western white pinePinus monticola420 lbf26.6 lb/ft³
White firAbies concolor480 lbf27.3 lb/ft³
White sprucePicea glauca410 lbf25.2 lb/ft³
Whitebark pinePinus albicaulis599 lbf*32.3 lb/ft³