Best wood for flooring
Compare wear, movement, installation method, and the room's conditions.

Which wood should you choose?
Oak is a versatile reference point for solid wood flooring. Hard maple provides a pale, firm surface, while hickory offers more pronounced variation and hardness. The right floor is a product and installation choice as well as a species choice; engineered construction may suit some sites better than solid boards.
Practical wood choices
These editorial choices account for the application as well as the numbers. They may differ from the automated property ranking below.
Oak
Readily available in many widths, grades, and factory finishes. White and red oak differ in appearance and properties. Compare the actual product and finishing system rather than treating oak as a single specification.
Species profiles:White oakNorthern red oak
Hard maple
A light-colored option with good dent resistance. Its fine, relatively quiet grain can make individual scratches and finish differences conspicuous. Test the intended stain and sheen on the supplied product.
Species profiles:Sugar mapleBlack maple
Hickory
A hard surface with strong grain and color variation. Movement and installation conditions deserve close attention. Buy enough consistent material and review a large sample layout rather than a single small board.
Species profiles:Shagbark hickory
What matters for this project
Janka measures indentation resistance; it does not measure scratch resistance of the finish, slip, acoustic performance, or suitability over heating. Board width, cut, construction, subfloor, and humidity all affect gapping and cupping. Decide on solid versus engineered flooring before using the species table to refine the choice.
What to check before you buy
Compare wear-layer thickness, finish, grade, moisture requirements, and approved installation methods. Check whether the product is intended for the room and subfloor. Review several boards for color variation and calculate waste from the actual layout. Keep spare matching material for future repairs.
Building and looking after it
Follow the flooring maker's acclimation, moisture testing, expansion, and fastening instructions. Address subfloor moisture and flatness before laying boards. Use suitable pads under furniture and remove abrasive grit. Clean with the product's recommended method rather than saturating the floor.
Mistakes to avoid
The hardest species is not automatically the best flooring. A premium dense board installed over an unsuitable subfloor can fail, while an appropriately specified ordinary floor may perform well. Green-to-dry shrinkage is not a prediction of a specific seasonal gap.
Property comparison ranking
The score combines Janka hardness divided by 4,000 with lower volumetric shrinkage at half weight.
This ranking compares selected properties. Use the practical choices above to check the other requirements of your project.
Species enter when the required fields are present and the rule gives a positive score. An absent wood may lack data or fall outside the scoring range; absence is not proof that it is unsuitable.
The order also uses an editorial availability multiplier, shown in the last column. It changes the order without removing a qualifying species. These scores compare selected properties; they do not evaluate every requirement of the finished project.
| # | Wood | Janka | Density | MOR | MOE | Shrinkage | T/R | Availability |
|---|---|---|---|---|---|---|---|---|
| 1 | Cocobolo | 3,860 lbf* | 69.0 lb/ft³ | — | — | 7.0% | 1.59 | |
| 2 | Ipe | 3,680 lbf | 70.0 lb/ft³ | 25,400 lb/in² | 3.14 ×10⁶ lb/in² | 13.2% | 1.21 | |
| 3 | Indian rosewood | 3,170 lbf | 53.0 lb/ft³ | 16,900 lb/in² | 1.78 ×10⁶ lb/in² | 8.5% | 2.15 | |
| 4 | Cumaru | 3,415 lbf | 66.8 lb/ft³ | 24,371 lb/in² | 2.43 ×10⁶ lb/in² | 13.5% | 1.56 | |
| 5 | Bubinga | 2,690 lbf | 55.9 lb/ft³ | 22,600 lb/in² | 2.48 ×10⁶ lb/in² | 14.2% | 1.45 | |
| 6 | Canalete | 2,200 lbf | 58.2 lb/ft³ | — | — | 11.6% | 1.85 | |
| 7 | Andaman Padauk | 1,630 lbf | 48.9 lb/ft³ | — | — | 6.4% | 1.33 | |
| 8 | Purpleheart | 1,860 lbf | 58.0 lb/ft³ | 19,200 lb/in² | 2.27 ×10⁶ lb/in² | 9.9% | 1.91 | |
| 9 | Brazilian rosewood | 2,720 lbf | 64.1 lb/ft³ | 19,000 lb/in² | 1.88 ×10⁶ lb/in² | 8.5% | 1.59 | |
| 10 | African Padauk | 1,538 lbf* | 46.0 lb/ft³ | 13,900 lb/in² | 1.56 ×10⁶ lb/in² | 7.6% | 1.58 | |
| 11 | Marishballi | 3,570 lbf | 62.0 lb/ft³ | 27,700 lb/in² | 3.34 ×10⁶ lb/in² | 17.2% | 1.56 | |
| 12 | Merbau | 1,500 lbf | 50.0 lb/ft³ | 16,800 lb/in² | 2.23 ×10⁶ lb/in² | 7.8% | 1.70 | |
| 13 | Azobe | 3,350 lbf | 70.0 lb/ft³ | 24,500 lb/in² | 2.47 ×10⁶ lb/in² | 17.0% | 1.31 | |
| 14 | Pecan hickory | 1,820 lbf | 46.1 lb/ft³ | 13,700 lb/in² | 1.73 ×10⁶ lb/in² | 13.6% | 1.82 | |
| 15 | Iroko | 1,260 lbf | 43.0 lb/ft³ | 12,400 lb/in² | 1.46 ×10⁶ lb/in² | 8.8% | 1.36 | |
| 16 | African ebony | 3,220 lbf | 63.0 lb/ft³ | 21,200 lb/in² | — | 20.0% | 1.17 | |
| 17 | Teak | 1,000 lbf | 40.0 lb/ft³ | 14,600 lb/in² | 1.55 ×10⁶ lb/in² | 7.0% | 2.32 | |
| 18 | Goncalo alves | 2,160 lbf | 67.7 lb/ft³ | 16,600 lb/in² | 2.23 ×10⁶ lb/in² | 10.0% | 1.90 | |
| 19 | Sucupira | 2,448 lbf* | 58.7 lb/ft³ | 19,400 lb/in² | — | 13.4% | 1.56 | |
| 20 | Shagbark hickory | 1,880 lbf | 50.3 lb/ft³ | 20,200 lb/in² | 2.16 ×10⁶ lb/in² | 16.7% | 1.50 | |
| 21 | Mockernut hickory | 1,970 lbf | 50.3 lb/ft³ | 19,200 lb/in² | 2.22 ×10⁶ lb/in² | 17.8% | 1.43 | |
| 22 | Wallaba | 2,040 lbf | 58.0 lb/ft³ | 19,100 lb/in² | 2.28 ×10⁶ lb/in² | 10.0% | 1.92 | |
| 23 | Rubberwood | 915 lbf* | 38.0 lb/ft³ | — | — | 7.4% | 2.22 | |
| 24 | Sapele | 1,510 lbf | 42.0 lb/ft³ | 15,300 lb/in² | 1.82 ×10⁶ lb/in² | 14.0% | 1.61 | |
| 25 | Bur oak | 1,370 lbf | 44.8 lb/ft³ | 10,300 lb/in² | 1.03 ×10⁶ lb/in² | 12.7% | 2.00 |
Before you choose a board
Use this ranking to compare the properties listed above. Grain direction, defects, moisture content, board dimensions, and construction also affect performance. Check the species page for the original measurements and any estimate marks, then inspect the actual stock you can buy.
The score does not assess decay resistance, food-contact suitability, heat resistance, or structural load capacity. For outdoor work, check durability and treatment requirements separately. For food-contact items and toys, check the intended finish and published safety information.
Read wood allergy and toxicity sourcesHow to read the measurements
Janka compares resistance to indentation. Density is the mass of a given volume of wood. Modulus of rupture (MOR) describes bending strength in a test specimen. Shrinkage figures describe the change from green to oven-dry wood, and T/R compares tangential with radial shrinkage. They are useful for comparison, but do not directly predict seasonal movement in your finished piece.
These are species-level reference values, not a test of the board you are buying or allowable structural design values. Grain, defects, moisture, dimensions, joints, and treatment can change the result. An asterisk beside Janka marks an estimate; open the species page for its source and method. Use the header settings to switch units.
Frequently asked questions
Will a harder floor resist every scratch?
No. Finish chemistry, grit, pet claws, and surface sheen influence scratching. Hardness mainly helps compare resistance to indentation under a standardized test.
Is engineered flooring always more stable?
Its layered construction can reduce some dimensional movement, but product quality and installation limits vary. Check the manufacturer's specification, including wear layer and site conditions.
How do I compare samples fairly?
View several full boards from the actual product under the room’s daylight and artificial lighting. Compare grain variation, sheen, edge profile, and finish texture alongside hardness. Ask about cleaning, repair, and refinishing requirements. A small perfect sample can hide the color range and grading features that will be obvious across an entire installed room.
Sources and further reading
The application advice is editorial guidance. The references below provide background; each wood's measured values have their own sources on its species page.
- USDA Forest Products Laboratory — Wood Handbook
Background on wood properties, moisture, construction, and finishing.