Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Abiurana-branca vs Grumixava

Micropholis mensalis against Micropholis spp.. Every number below names the publication it came from.

PropertyAbiurana-brancaGrumixava
Janka hardness1,605 lbfLPF/SFB Madeiras Brasileiras1,490 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC46.2 lb/ft³LPF/SFB Madeiras Brasileiras46.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture17,423 lb/in²LPF/SFB Madeiras Brasileiras18,890 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.95 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.95 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength8,377 lb/in²LPF/SFB Madeiras Brasileiras9,820 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)14.7%LPF/SFB Madeiras Brasileiras14.3%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.85LPF/SFB Madeiras Brasileiras1.47Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.