Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Abiurana vs Tuturubá

Pouteria sp against Pouteria gongrijpii = Franchetella gongrijpii. Every number below names the publication it came from.

PropertyAbiuranaTuturubá
Janka hardness2,418 lbfLPF/SFB Madeiras Brasileiras2,396 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC57.4 lb/ft³LPF/SFB Madeiras Brasileiras56.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture22,516 lb/in²LPF/SFB Madeiras Brasileiras20,951 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.45 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.22 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,436 lb/in²LPF/SFB Madeiras Brasileiras10,952 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)15.2%LPF/SFB Madeiras Brasileiras15.0%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.64LPF/SFB Madeiras Brasileiras2.24LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.