Abiurana-seca vs Cumaru

Diploon cuspidatum = Diploon venezuelana against Dipteryx odorata. Every number below names the publication it came from.

PropertyAbiurana-secaCumaru
Janka hardness2,945 lbfLPF/SFB Madeiras Brasileiras3,415 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC68.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-966.8 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture27,109 lb/in²LPF/SFB Madeiras Brasileiras24,371 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.57 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.43 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength13,982 lb/in²LPF/SFB Madeiras Brasileiras14,742 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)15.7%LPF/SFB Madeiras Brasileiras13.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.42LPF/SFB Madeiras Brasileiras1.56LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.