PropertyAfrican PadaukAndaman Padauk
Janka hardness1,538 lbfEstimateUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11a1,630 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC46.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)48.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture13,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Modulus of elasticity1.56 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Crushing strength8,450 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Volumetric shrinkage(lower is better)7.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)6.4%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.58Chudnoff 1984, Tropical Timbers of the World (AH-607)1.33Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons