Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Agba vs African mahogany

Gossweilerodendron balsamiferum against Khaya spp.. Every number below names the publication it came from.

PropertyAgbaAfrican mahogany
Janka hardness740 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)830 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC30.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)32.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture11,800 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)10,700 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.10 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.40 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength6,270 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)6,460 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)—8.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)—1.80USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.