Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Amapá-doce vs Mururé

Brosimum potabile against Brosimum acutifolium subsp interjectum. Every number below names the publication it came from.

PropertyAmapá-doceMururé
Janka hardness1,184 lbfLPF/SFB Madeiras Brasileiras1,120 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC40.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-942.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture14,095 lb/in²LPF/SFB Madeiras Brasileiras14,508 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.56 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.69 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength7,980 lb/in²LPF/SFB Madeiras Brasileiras7,922 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)11.9%LPF/SFB Madeiras Brasileiras12.6%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.66LPF/SFB Madeiras Brasileiras1.63LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.