American elm vs Yellow-poplar

Ulmus americana against Liriodendron tulipifera. Every number below names the publication it came from.

PropertyAmerican elmYellow-poplar
Janka hardness830 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b540 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC35.0 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b29.3 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture11,800 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b10,100 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity1.34 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1.58 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength5,520 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b5,540 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)14.6%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-312.7%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)2.26USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-31.78USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • manual map (regional variant)public domain