Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Amora / amoreira vs Canalete

Maclura tinctoria against Cordia spp. (hard-wooded, dark-colored Gerascanthus group). Every number below names the publication it came from.

PropertyAmora / amoreiraCanalete
Janka hardness2,385 lbfLPF/SFB Madeiras Brasileiras2,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC56.8 lb/ft³LPF/SFB Madeiras Brasileiras58.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture22,259 lb/in²LPF/SFB Madeiras Brasileiras—
Modulus of elasticity1.83 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras—
Crushing strength12,488 lb/in²LPF/SFB Madeiras Brasileiras—
Volumetric shrinkage(lower is better)9.4%LPF/SFB Madeiras Brasileiras11.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.84LPF/SFB Madeiras Brasileiras1.85Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.